MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Crosspolimeri FRAGOM G/830 R Flame Retardant Halogen Free Polyolefine
Categories: Polymer; Thermoplastic; Polyolefin

Material Notes: FRAGOM: is the trade-mark of our flame retardant and halogen free polyolefin compounds

FRAGOM G/830 R: halogen-free flame-retardant crosslinked compound suitable for thin wall automotive cables and low voltage insulation. To be used with 5 % of catalyst MAC/203 HSL The material is suitable to use as insulation on cables size >/= 1,5 mm2. Exercise temperature: - 40 / +125°C

Certify: SAE J1127/J1128,FIAT 7.Z8220 T3 ,ISO 6722 Class C, LV 112 Class C

Information provided by Crosspolimeri S.P.A.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Melt Flow 30 g/10 min
@Load 21.6 kg,
Temperature 190 °C
30 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Storage Temperature 12.0 °C53.6 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 6060ASTM D2240
Tensile Strength >= 12.5 MPa>= 1810 psiIEC 60811
Elongation at Break 120 %120 %IEC 60754-2
 
Thermal PropertiesMetricEnglishComments
Oxygen Index 28 %28 %ASTM D2863
 
Processing PropertiesMetricEnglishComments
Zone 1 90.0 - 100 °C194 - 212 °F
Zone 2 110 - 120 °C230 - 248 °F
Zone 3 150 °C302 °F
Zone 4 165 °C329 °F
Die Temperature 180 °C356 °F
Head Temperature 175 °C347 °F
Dry Time 4.00 hour
@Temperature 80.0 °C
4.00 hour
@Temperature 176 °F
 
Descriptive Properties
Exercise temperature-40 - 125°C
Hot Set Test0.5200°C - 20 N/cm2, IEC 60811

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCROS065 / 294149

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.