MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives CoolTherm™ SC6711/6732 Silicone Encapsulant
Categories: Polymer; Thermoset; Silicone; Silicone Elastomer, for Thermal Management

Material Notes: LORD CoolTherm™ SC-6711/6732 silicone encapsulant is a two-component, thermally conductive encapsulant system with outstanding electrical properties. CoolTherm SC-6711/6732 encapsulant system is an ideal potting compound for any application where rapid heat transfer, high temperature service and a flexible system are required.

Features: maintains low viscosity for complete and void-free encapsulation. provides thermal conductivity for applications where superior heat dissipation are required. minimizes the possibility of cracking during severe temperature cycling.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.15 g/ccSC-6732 Hardener
 2.20 g/ccSC-6711 WHT Silicone Resin
Viscosity 350 cP
@Temperature 25.0 °C
SC-6732 Hardener
 30000 cP
@Temperature 25.0 °C
SC-6711 WHT Silicone Resin
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60cured
Tensile Strength 800 psi
@Temperature 25.0 °C
cured
Elongation at Break 70 %cured
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cm
@Temperature 25.0 °C
cured
Dielectric Constant 5.2cured
Dielectric Strength 500 V/milcured
Dissipation Factor 0.020cured
 
Thermal PropertiesOriginal ValueComments
CTE, linear 150 µm/m-°Ccured
Thermal Conductivity 1.00 W/m-Kcured, hot die transient method
 
Processing PropertiesOriginal ValueComments
Cure Time 6.00 - 8.00 hour
@Temperature 25.0 °C
mixed
Pot Life <= 30.0 min
@Temperature 25.0 °C
mixed, working life
Shelf Life 6.00 Month
@Temperature 25.0 °C
SC-6711 WHT Silicone Resin, from date of manufacture when stored in original, unopened container
 12.0 Month
@Temperature 25.0 °C
SC-6732 Hardener, from date of manufacture when stored in original, unopened container
 
Descriptive Properties
AppearanceAmber LiquidSC-6732 Hardener
 White PasteSC-6711 WHT Silicone Resin
Usage Level % by weight0.5mixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lord Adhesives CoolTherm™ SC-6709/6730 Silicone encapsulant system
Lord Adhesives CoolTherm™ SC-6710/6731 Silicone Resin System
Lord Adhesives CoolTherm™ SC6711/6730 Silicone Encapsulant
Lord Adhesives CoolTherm™ SC6711/6731 Silicone Encapsulant
Lord Adhesives CoolTherm™ SC-6712/6730 Silicone Resin System

PLORD9244 / 232600

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.