MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Inov Chem 910R Polyurethane resin
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane TPE

Material Notes: Introduction: 910R is a silane modified polyurethane resin based on high molecular weight polyether, end-capped with siloxane and containing carbamate groups, has the characteristics of high activity, no dissociative isocyanate, no solvent, excellent adhesion and so on. 910R curing mechanism is moisture curing. Catalysts are needed in sealant formulation. Ordinary organotin catalysts (such as dibutyltin dilaurate) or chelated tin (such as diacetylacetone dibutyltin) can achieve good mechanical properties. The recommended amount of tin catalysts is 0.2-0.6%. 910R resin combinated with plasticizer, nano-calcium carbonate, silane coupling agent and other fillers and additives can prepare sealant products which has tensile strength of 1.0-4.0 MPa, 100% modulus between 0.3-2.0 MPa and elastic recovery of more than 70%. 910R can also be used to prepare transparent sealants which are widely used in building exterior wall, home decoration, industrial elastic sealant, elastic adhesive and so on

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.960 - 1.04 g/cc0.960 - 1.04 g/cc
pH 6.0 - 8.06.0 - 8.0Isopropanol/aqueous solution
Brookfield Viscosity 50000 - 70000 cP50000 - 70000 cP
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %Karl Fischer
 
Descriptive Properties
AppearanceColorless to pale yellow transparent viscous liquid
Color<50APHA

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM042 / 312571

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.