System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Lotte Advanced Materials MEG (Mono Ethylene Glycol) Plant: YEOSU
Categories:
Fluid
Material Notes:
Low viscosity, Low freezing-point
Applications: Raw materials for polyester fibers and films, Automotive antifreeze, and Refrigerant
Information provided by Lotte Advanced Materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.1151
-
1.1156
g/cc
0.040286
-
0.040304
lb/in³
ASTM D4052
Ash
<= 0.000500 %
<= 0.000500 %
ASTM D482
Thermal Properties
Metric
English
Comments
Distillation Temperature
196.5
-
198.5
°C
385.7
-
389.3
°F
5% TO 95% Range; ASTM E202
Optical Properties
Metric
English
Comments
UV Transmittance
>= 81.4 %
@Wavelength 220 nm
>= 81.4 %
@Wavelength 220 nm
SMS 1997
>= 93.3 %
@Wavelength 260 nm
>= 93.3 %
@Wavelength 260 nm
SMS 1997
Descriptive Properties
Acidity
<50 ppm
as Acetic Acid; ASTM E202
Color
<10 APHA
ASTM D1209
Content
<0.05%
Diethylene Glycol; ASTM E202
<0.2 ppm
Iron; ASTM E202
<1.0 ppm
Chloride (as NaCl); JIS K1527
<500
Water; ASTM E202
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PLOTT9316 / 325798
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.