MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Moplen HP555G Polypropylene, Extrusion Grade
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Extrusion Grade

Material Notes: LyondellBasell Australia’s Polypropylene grade HP555G is a low flow homopolymer with a conventional molecular weight distribution and is formulated with an enhanced process stability additive package. HP555G is designed for extrusion processes that demand high melt strength and melt stability characteristics. End use products typically made from HP555G include strapping, mechanically fibrillated yarns and profiles. Applications: Panels & Profiles, Strapping.

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.900 g/ccISO 1183-1
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133-1
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 75ISO 868
Tensile Strength, Yield 33.0 MPaISO 527-1,-2
Flexural Modulus 1450 MPaISO 178
Izod Impact, Notched (ISO) 7.50 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 92.0 °Cunannealed; ISO 75B-1,-2
Vicat Softening Point 155 °CISO 306
 
Descriptive Properties
Processing MethodExtrusion blow molding, sheet

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Pro-fax EP424E Polypropylene, Extrusion Grade
LyondellBasell Moplen HP555E Polypropylene, Extrusion Grade

PEQT9050 / 220681

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.