MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Inov Chem GPEG3000 Polycarboxylate Superplasticier Macro-monomer(PC)–GPEG
Categories: Polymer

Material Notes: Characteristic & Application: This series of products are non-toxic, non-irritating and are important raw materials for functional polycarboxylate superplasticizer. The quality of these products are very stable when stored reasonable. Due to the special molecular structure, the space resistance of the polyether side chain is reduced, the swing of the side chain is more free, and the encapsulation and entanglement of the polyether side chain is improving. Polycarboxylate superplasticizer with excellent slump retention and good adaptability is formed by this series of macro-monomer copolymerize with acrylic acid. The synthesized PCE has good dispersibility and slump retention, high adaptability, high early strength and good viscosity reducing effects. It is especially suitable for projects using poor grave, poor cement or with high requirements for concrete.

Speciality: Excellent slump retention, excellent adaptability, good viscolity reducing effects

Information provided by Shandong INOV Polyurethane Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
pH 10 - 1210 - 121% aqueous solution
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.50 %<= 0.50 %
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
AppearanceWhite to light yellow solid, slice
Color<200Pt-Co, 10% solution, Hazen
OH value17-19 mg KOH/g
Purity=94%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PINOVCHM062 / 312591

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.