MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

SABIC LNP™ THERMOCOMP™ HF008 Nylon 11 (Global)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 11 (PA11)

Material Notes: LNP THERMOCOMP* HF008 is a compound based on Nylon 11 resin containing 40% Glass Fiber.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.37 g/cc0.0495 lb/in³ASTM D792
 1.37 g/cc0.0495 lb/in³ISO 1183
Moisture Absorption 0.100 %0.100 %50% RH, 24 hrs; ASTM D570
 0.190 %0.190 %23°C / 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24HRS; ASTM D955
 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/in24HRS; ISO 294
Linear Mold Shrinkage, Transverse 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/in24 HRS; ASTM D955
 0.0080 - 0.010 cm/cm0.0080 - 0.010 in/in24 HRS; ISO 294
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 122 MPa17700 psiASTM D638
 123 MPa17800 psiISO 527
Elongation at Break 3.9 %3.9 %ISO 527
 4.9 %4.9 %ASTM D638
Tensile Modulus 7.60 GPa1100 ksi1 mm/min; ISO 527
 9.28 GPa1350 ksi50 mm/min; ASTM D638
Flexural Strength 192 MPa27800 psiISO 178
 220 MPa31900 psiASTM D790
Flexural Modulus 7.97 GPa1160 ksiISO 178
 8.48 GPa1230 ksiASTM D790
Izod Impact, Notched 2.40 J/cm4.50 ft-lb/inASTM D256
Izod Impact, Unnotched 12.28 J/cm23.01 ft-lb/inASTM D4812
Izod Impact, Notched (ISO) 21.0 kJ/m²9.99 ft-lb/in²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 75.0 kJ/m²35.7 ft-lb/in²80*10*4; ISO 180/1U
Impact Test 3.00 J2.21 ft-lbMultiaxial Impact; ISO 6603
Instrumented Impact Energy at Peak 18.0 J13.3 ft-lbASTM D3763
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  28.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 30.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
16.9 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  88.2 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.0 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 88.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
49.3 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 175 °C347 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 177 °C
@Thickness 3.20 mm
351 °F
@Thickness 0.126 in
unannealed; ASTM D648
 
Processing PropertiesMetricEnglishComments
Zone 1 200 - 210 °C392 - 410 °F
Zone 2 230 - 245 °C446 - 473 °FInjection Molding
Zone 3 260 - 270 °C500 - 518 °F
Melt Temperature 225 - 260 °C437 - 500 °FInjection Molding
Mold Temperature 45.0 - 55.0 °C113 - 131 °F
Drying Temperature 80.0 °C176 °FInjection Molding
Dry Time 4.00 hour4.00 hourInjection Molding
Moisture Content 0.15 %0.15 %Injection Molding
Back Pressure 0.200 - 0.300 MPa29.0 - 43.5 psi
Screw Speed 30 - 60 rpm30 - 60 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH92209 / 253333

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.