MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SEKISUI SPI ALLEN® 5100WHG ASA/ABS Sheet
Categories: Polymer; Thermoplastic; ABS Polymer; ASA Polymer

Material Notes: ALLEN® 5100WHG is high impact ABS capped with medium gloss ASA for UV protection.

ALLEN® 5100WHG has been tested under laboratory conditions and has achieved a UL94 HB rating at 0.060 in (1.52mm) and above and meets the requirements of Federal Motor Vehicle Safety Standard No. 302 (FMVSS 302).

Suggested Application:

  • Vehicle Exterior
  • Radomes
  • Bus Hatches
  • Sunroom Exterior & Interiors
  • Equipment Housings
  • Marine Dashes & Components
Features:
  • Custom color matching
  • Excellent UV properties
  • Edge trim easily used into future orders
  • Medium gloss finish

Information provided by SEKISUI KYDEX, LLC.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.05 g/ccASTM D792
Water Absorption 0.370 %equilibrium; ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 40.3 MPaASTM D638
Tensile Modulus 88.3 MPaASTM D638
Flexural Strength 61.9 MPa
@Strain 5.00 %
ASTM D790
Flexural Modulus 2040 MPaASTM D790
Compressive Yield Strength 48.8 MPaASTM D695
Bearing Yield Strength <= 177.2 MPaASTM D953
 20.2 MPa
@Strain 4.00 %
ASTM D953
Shear Strength 30.6 MPaASTM D732
Izod Impact, Notched 390 J/mASTM D256
Gardner Impact 37.3 JDrop Dart Impact, GE; ASTM D5420
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 18.1 kV/mmoil; ASTM D149
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 94.7 µm/m-°CASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 90.6 °Cannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 79.4 °Cannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSEKIS540 / 325280

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.