MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Geon® Performance Solutions Duracap™ 86103 PVC, Flexible  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D792
Water Vapor Transmission 16.0 g/m²/day1.03 g/100 in²/dayInternal Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 72
@Time 15.0 sec
72
@Time 0.00417 hour
ASTM D2240
Film Tensile Strength at Yield, MD 20.7 MPa3000 psiASTM D882
Film Tensile Strength at Yield, TD 20.7 MPa3000 psiASTM D882
Film Elongation at Break, MD 200 %200 %ASTM D882
Film Elongation at Break, TD 200 %200 %ASTM D882
Film Elongation at Yield, MD 3.0 %3.0 %ASTM D882
Film Elongation at Yield, TD 3.0 %3.0 %ASTM D882
Tear Strength 87.6 kN/m500 pliDie C, 2 in/min; ASTM D1004
Film Tensile Strength at Break, MD 27.6 MPa4000 psiASTM D882
Film Tensile Strength at Break, TD 27.6 MPa4000 psiASTM D882
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 98.0 kV/mm2490 kV/inASTM D149
 
Thermal PropertiesMetricEnglishComments
Shrinkage  1.0 %
@Temperature 80.0 °C
1.0 %
@Temperature 176 °F
10 in square in hot oven, 10 min, Flow; ASTM D1042
 2.0 %
@Temperature 130 °C
2.0 %
@Temperature 266 °F
10 in square in hot oven, 10 min, Flow; ASTM D1042
 50 %
@Temperature 200 °C
50 %
@Temperature 392 °F
10 in square in hot oven, 10 min, Flow; ASTM D1042
Shrinkage, TD  2.0 %
@Temperature 80.0 °C
2.0 %
@Temperature 176 °F
10 in square in hot oven, 10 min, Across Flow; ASTM D1042
 7.0 %
@Temperature 130 °C
7.0 %
@Temperature 266 °F
10 in square in hot oven, 10 min, Across Flow; ASTM D1042
 30 %
@Temperature 200 °C
30 %
@Temperature 392 °F
10 in square in hot oven, 10 min, Across Flow; ASTM D1042
 
Optical PropertiesMetricEnglishComments
Gloss 15 - 45 %15 - 45 %60°; Gardner Gloss; ASTM D523
 
Processing PropertiesMetricEnglishComments
Melt Temperature 177 - 188 °C351 - 370 °F
 
Descriptive Properties
FeaturesLow Gloss
FormsCube
Processing MethodCoextrusion
 Encapsulating
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesCapstock
 Outdoor Applications
 Profiles
 Siding Capstock
 Windows & Doors

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for PVC, Wire and Cable Grade
Geon® Performance Solutions W1101 Wire & Cable PVC
Geon® Performance Solutions Vinyl Wire & Cable W9200 Polyvinyl Chloride, Flexible
Axiall 21540 Coax & Telecom Flexible PVC

PH1PN8171 / 102007

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.