Moplen EP300R is a polypropylene impact copolymer with optimized balance of stiffness and toughness, and high impact strength even at low temperature. Typical customer applications are injection molding of washing machine tubs, electrical appliance parts, house wares and thin walled packaging. Applications: House wares, TWIM Food Containers, TWIM Non-food ContainersInformation provided by LyondellBasell. |