MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Latrobe LSS™ H10A Modified
Categories: Metal; Ferrous Metal; Alloy Steel; Chrome-moly Steel; Tool Steel; Hot Work Steel

Material Notes: TLS H10 Mod. hot work tool steel is a chromium-molybdenum H10-type hot work steel which contains cobalt for increased strength and resistance to softening at elevated temperature. This grade is also very resistant to thermal fatigue cracking (heat checking), and can be water cooled in service. TLS H10 Mod. is recommended for difficult hot work tooling applications such as hot punches, die casting dies, forging dies, hot shear blades, hot gripper dies, and extrusion tooling.

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.281 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell C 32Air Cooled from 1010°C; 650°C Temper Temperature
 33Oil Quenched from 1010°C; 650°C Temper Temperature
 35Air Cooled from 1066°C; 650°C Temper Temperature
 35Oil Quenched from 1066°C; 650°C Temper Temperature
 54.5Oil Quenched from 1010°C; 482°C Temper Temperature
 55Air Cooled from 1010°C; 482°C Temper Temperature
 56.5Air Cooled from 1066°C; 482°C Temper Temperature
 59.5Oil Quenched from 1066°C; 482°C Temper Temperature
Modulus of Elasticity 30000 ksi
Machinability 90 - 95 %1% Carbon Steel
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.3 µm/m-°C
@Temperature 21.0 - 204 °C
 13.5 µm/m-°C
@Temperature 21.0 - 538 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 830 °CCritical Temperaure Ac1
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.35 %
Chromium, Cr 3.3 %
Cobalt, Co 2.0 %
Iron, Fe 89.95 %
Manganese, Mn 0.30 %
Molybdenum, Mo 2.45 %
Silicon, Si 1.0 %
Vanadium, V 0.65 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Corundum, Aluminum Oxide, Alumina, 99.9%, Al2O3
Tungsten Carbide, WC
AISI Type H13 Hot Work Tool Steel
Industeel CLC 1.2312 Prehardened Mold Steel (300HB/32HRC) with Improved Machinability
International Mold Steel TOOLOX® 33 Cold Work Die Steel

NTIMK080 / 19427

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.