MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Phillips 66 Syncon® Barrier Oil SO Grade 5
Categories: Fluid; Lubricant; Polyalphaolefin (PAO)

Material Notes: Syncon Barrier Oil is a premium quality, non-reactive, synthetic, low-viscosity process oil developed for use as a barrier oil in seal applications where the manufacturer calls for a light mineral seal oil. Typical applications include seal service in refineries, gas plants, steel mills, power plants and chemical plants. Syncon Barrier Oil is manufactured with synthetic polyalphaolefin (PAO) base oils and select additives to provide excellent oxidation inhibition and lubricity over a wide temperature range. It is free of impurities that can cause catalyst poisoning in process applications, and is compatible with most commonly used sealmaterials. It complies with FDA 21 CFR 178.3570 regulations for use in food processing plants where there is the possibility of incidental food contact.

Applications:

  • Seal applications in gas processing and pumping
  • Barrier fluid in dual mechanical seals used in refineries, power plants and chemical plants, where the manufacturer calls for a premium quality light mineral seal oil
Features/Benefits:
  • Premium quality seal oil
  • Outstanding oxidation resistance and thermal stability at high temperatures
  • Superior heat transfer properties
  • Excellent low-temperature fluidity
  • Resistant to chemical contamination
  • Helps keep the face of the seal cool and free of deposits
  • Low odor

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.797 g/cc
Density 6.64 lb/gal
Saybolt Viscosity at 100°F 43.7 SUS
Saybolt Viscosity at 210°F 31.9 SUS
Kinematic Viscosity at 40°C (104°F) 5.1 cSt
Kinematic Viscosity at 100°C (212°F) 1.7 cSt
Oxidative Stability 40 hourRPVOT; ASTM D2272
ASTM Color 0.50ASTM D1500
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 0.17[mg KOH/g]; ASTM D974
 
Mechanical PropertiesOriginal ValueComments
Four Ball Wear 0.550 mmScar Diameter; ASTM D4172
 
Thermal PropertiesOriginal ValueComments
Pour Point -60.0 °C
Flash Point 149 °CCOC
 
Compliance PropertiesOriginal ValueComments
FDA Yes
 
Descriptive Properties
Copper Corrosion1aASTM D130
Demulsibility10 minutes to passASTM D1401

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5234 / 198487

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.