Microthene G polyolefin powders are ground, irregularly-shaped particles for use in a broad range of specialty applications. Microthene G powders combine the properties of a polyolefin resin with a small ground particle size. Applications: Automotive Parts, Color Concentrates, Industrial, Interior Automotive Applications, Structural Parts.Information provided by LyondellBasell. |