MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Osterman & Co Osterlene® HB1049 Extra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Product Description: An extra high molecular weight hexane copolymer. It has good melt strength, good rigidity, excellent stress crack resistance and excellent impact strength even at low temperatures. HB1049 is excellent for large part molding applications. Recommended applications for HB1049 include blow molding large shipping containers, agricultural chemical tanks and gasoline tanks. Extruded applications would include pallets, cattle feeders, large formed parts and boats.

Availability: North America
Features: Copolymer; Good Melt Strength; Good Rigidity; High ESCR (Stress Crack Resist.); High Impact Resistance; Low Temperature Impact Resistance
Uses: Agricultural Applications; Agricultural Tanks; Containers; Fuel Tanks; Pallets
Processing Method: Blow Molding; Extrusion

Information provided by Osterman & Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.949 g/cc0.0343 lb/in³ASTM D792
ESCR 100% Igepal® >= 600 hour>= 600 hourF50; ASTM D1693A
ESCR 10% Igepal® >= 600 hour>= 600 hourF50; ASTM D1693B
Melt Flow 10 g/10 min
@Load 21.6 kg,
Temperature 190 °C
10 g/10 min
@Load 47.6 lb,
Temperature 374 °F
Conditioned F; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 24.8 MPa
@Thickness 50.8 mm
3600 psi
@Thickness 2.00 in
ASTM D638
Elongation at Yield >= 600 %
@Thickness 50.8 mm
>= 600 %
@Thickness 2.00 in
ASTM D638
Flexural Modulus 1.17 GPa170 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -91.1 °C<= -132 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POSTER022 / 267604

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.