MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Techmer ES HiFill FR® PA6/6 GF25 FR NAT003 25% Glass Filled (Conditioned)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled; Nylon 66, Heat Stabilized

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Glass Fiber, 25% Filler by Weight

Additive: Heat Stabilizer and Lubricant

Features: Flame Retardant, Heat Stabilized and Lubricated

UL File Number: E157318

Appearance: Natural Color

TPCI# 8230101

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ASTM D792
Water Absorption 0.60 %
@Time 86400 sec
0.60 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 3.17 mm
0.0030 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ASTM D785
Tensile Strength, Yield 123 MPa17900 psiASTM D638
Elongation at Break 4.0 %4.0 %ASTM D638
Flexural Strength 174 MPa25200 psiASTM D790
Flexural Modulus 6.55 GPa950 ksiASTM D790
Izod Impact, Notched 1.28 J/cm
@Thickness 3.17 mm
2.40 ft-lb/in
@Thickness 0.125 in
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polypropylene with 20% Glass Fiber Filler
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned)
LyondellBasell Hostacom ERG 393F C1 BLACK Polypropylene with 20% Glass Fiber Filler
LyondellBasell Hostacom ERG 393F BLACK Polypropylene with 20% Glass Fiber Filler
Celanese Celstran® PP-GF20-02 AD 3002 PP, 20% Glass Reinforced

PTPC0701 / 136639

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.