MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos N01N-00 Polypropylene Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Grade N01N-00 is a high stiffness, impact copolymer specially designed for freezer-to-microwave performance. This extrusion grade resin exhibits an excellent balance of impact and stiffness properties, and combines high heat resistance with good gloss and thermoformability. This grade meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.
    Applications:
  • Food service trays, containers
  • Rigid packaging
    Benefits:
  • Very broad temperature performance range
  • High stiffness
  • Low temperature impact
  • Thermoformability

Key Words: Excellent balance of impact and stiffness properties
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.908 g/cc0.0328 lb/in³ASTM D792
Melt Flow 1.9 g/10 min
@Load 2.16 kg,
Temperature 230 °C
1.9 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9595ASTM D785
Tensile Strength at Break 15.2 MPa2210 psi2.0 in/min, Injection Molded; ASTM D638
Tensile Strength, Yield 30.1 MPa4360 psi2.0 in/min, Injection Molded; ASTM D638
Elongation at Break 150 %150 %2.0 in/min, Injection Molded; ASTM D638
Elongation at Yield 6.5 %6.5 %2.0 in/min, Injection Molded; ASTM D638
Flexural Modulus, 1% Secant 1620 MPa235000 psiInjection Molded; ASTM D790A
Izod Impact, Notched 0.534 J/cm
@Temperature -20.0 °C
1.00 ft-lb/in
@Temperature -4.00 °F
Injection Molded; ASTM D256
Izod Impact, Notched (ISO)  5.29 kJ/m²
@Temperature -20.0 °C
2.52 ft-lb/in²
@Temperature -4.00 °F
Area; ASTM D256
 NB
@Temperature 22.8 °C
NB
@Temperature 73.0 °F
Area; ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 111 °C231 °FUnannealed, Injection Molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.6 °C141 °FUnannealed, Injection Molded; ASTM D648
Vicat Softening Point 154 °C309 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Gloss 75 %75 %60°, Injection Molded; ASTM D2457
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.
 
Descriptive Properties
ProcessExtrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ineos N02G-00 Polypropylene Impact Copolymer
Ineos N02J-00 Polypropylene Impact Copolymer
Ineos N01G-02 Polypropylene Impact Copolymer
Formosa Plastics Formolene® 2302E Impact Copolymer Polypropylene
Ineos N00G-01 Polypropylene Impact Copolymer

PINEOS902 / 104595

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.