MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
LyondellBasell Astryn BA905-74 Polypropylene Copolymer, Flame Retardant  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Key Features: medium high melt flow, medium high modulus, flame retardant, low specific gravity, good impact strength

Applications: battery jars, electrical components

Description: Astryn BA905-74 medium high melt flow, UL 94 V-0 flame retardant polypropylene copolymer has a very good combination of properties and processability. It was designed for applications which have stringent flammability requirements.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.04 g/ccASTM D792B
Linear Mold Shrinkage 0.014 cm/cmTool, Montell
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 93ASTM D785
Tensile Strength, Yield 32.0 MPaASTM D638
Elongation at Break 225 %ASTM D638
Flexural Modulus, 1% Secant 1.50 GPa0.05 in/min; ASTM D790A
Izod Impact, Notched 0.430 J/cmASTM D256A
Gardner Impact 2.00 JASTM D3029
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 85.0 °CASTM D648
Flammability, UL94 V-0
@Thickness 1.50 mm
Oxygen Index 30 %ASTM D2863

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Tipco Tipcolene® FX 4000 - UL94-V0 Flame Retardant Polypropylene Copolymer, High Impact Strength
LG Chemical LUPOL GP-1000FA General Purpose Polypropylene, High Impact, Flame Retardant, Non-Bleed
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant
Aurora Plastics GPP1001V0M-HCO PP
Avient Maxxam™ FR PP 402 Polypropylene

PMO429 / 53632

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.