This material meets FDA regulation CFR 21 177.1520 and is suitable for food packaging applications.Applications: - Bulked continuous filament
- Craft yarn
- Nonwoven fabrics
Information provided by Chevron Phillips. Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. |