MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Akrochem Akrosorb® 19480
Categories: Other Engineering Material

Material Notes: Product Description: Akrosorb 19480 is a 75% active dispersion of SR 206 on calcium silicate (crystalline quartz-free). SR 206 is Ethylene Glycol Dimethacrylate, a difunctional peroxide co-agent. Because SR 206 is a liquid normally used in smaller quantities, this non-dusting, free-flowing powder aids weigh-up and batch addition.

Applications: Akrosorb 19480 is an efficient peroxide coagent for curing of most elastomeric systems. As little as 2 phr of active material will raise the modulus and hardness as well as improve compression set resistance (essentially increasing cross-link density). Alternately, less peroxide needs to be used to reach an equivalent state-of-cure of a formula using peroxide alone. Higher levels of 19480 will continue to raise hardness and modulus while at the same time plasticizing the rubber. High hardness compounds (70 Shore D) can be made that have excellent processibility and better elastomeric properties (compression set resistance) than filler or plastic reinforced rubber. It is advisable to use a scorch-retarded coagent (such as SR 500 or 516) when using high levels of acrylate coagents. In contrast to other coagent types, the acrylic resin monomer is useful in all peroxide curable rubbers.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.22 g/cc
 
Descriptive Properties
Active0.05
Appearancetan powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH547 / 315465

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.