MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Milliken® Hyperform® HPR-803i Reinforcing Agent for Polyolefins
Categories: Ceramic; Other Engineering Material; Composite Fibers

Material Notes: Hyperform® HPR-803i enables high performance polyolefin compounds with reduced densities when compared to traditional fillers. A synthetic, mineral-based fiber, HPR-803i allows for excellent stiffness/impact balance and reduced part weight. In addition, improved surface quality, scratch performance and color response can offer valuable aesthetic benefit in high quality interior applications.

Hyperform HPR-803i Attributes:

  • Lighter weight parts
  • Improved scratch resistance
  • Excellent surface finish
  • Higher stiffness and improved HDT

Information provided by Milliken®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.953 g/cc0.0344 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Flexural Modulus, 1% Secant  2000 MPa
@Strain 4 %
290000 psi
@Strain 4 %
ASTM D790
 4000 MPa
@Strain 16 %
580000 psi
@Strain 16 %
ASTM D790
 6000 MPa
@Strain 25 %
870000 psi
@Strain 25 %
ASTM D790
Charpy Impact, Notched 3.90 J/cm²18.6 ft-lb/in²ASTM D6110

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Milliken® Hyperform® HPN-600ei Nucleating Agent for Polypropylene
Milliken® Hyperform® HPN-20E Nucleating Agent for Polypropylene

PMILLIK017 / 194988

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.