MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Thermal Ceramics Kao-Tex A-54 HT 1900 Cloth
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Kao-Tex 1900 Cloths are a specially processed silica fabric having much improved high-temperature properties over our Kao-Tex 1800 silica textiles. This textile has unique properties of higher strength retention and maintained flexibility after exposure for long periods to temperatures as high as 1900°F.

Kao-Tex 1900 is available in both standard and pre-shrunk grades. The standard grade will have a hydrocarbon coating to improve handling and abrasion properties. The pre-shrunk grades (B-30 HTS and A-54 HTS) are available with the following choices: no coating; hydrocarbon coating; or a special coating to give improved drapeability, tear strength, and adhesion properties when used in reinforced composites. Coatings of silicone, neoprene, or aluminization can be applied to Kao-Tex 1900.

Features:

  • Made from high silica yarn
  • Easily sewn and fabricated
  • High strength and flexibility
  • Information provided by Thermal Ceramics

    Data has not been recently verified. Please contact manufacturer for current information.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Thermal PropertiesOriginal ValueComments
    Melting Point 3000 °F
    Maximum Service Temperature, Air 1800 °F
    Shrinkage 10 %Residual
     
    Component Elements PropertiesOriginal ValueComments
    Al2O3 0.071 %
    B2O3 >= 0.016 %
    CaO 0.023 %
    MgO >= 0.017 %
    SiO2 97.85 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

    CTHERM308 / 2628

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.