MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

HB Fuller Advantra® PHC8290 Hot melt adhesive
Categories: Polymer; Adhesive

Material Notes: Type of Product: Hot melt adhesive

Product Characteristics:

  • fast speed of setting
  • robust adhesion
  • low color
  • low odor
  • smoke-free environment
  • increased mileage
  • clean machining
Typical Applications: Cases, cartons, trays, Bliss Box, high spring-back containers

Suitable Substrates: Uncoated, clay coated, SBS, SUS, and similar uncoated and lightly coated materials

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.970 g/cc0.970 g/cc
Viscosity  800 cP
@Temperature 191 °C
800 cP
@Temperature 375 °F
 900 - 1220 cP
@Temperature 177 °C
900 - 1220 cP
@Temperature 350 °F
 1515 cP
@Temperature 163 °C
1515 cP
@Temperature 325 °F
Storage Temperature 20.0 - 100 °C68.0 - 212 °F
 
Thermal PropertiesMetricEnglishComments
Softening Point 102 - 113 °C215 - 235 °FMettler
 
Optical PropertiesMetricEnglishComments
Gardner Color Number 1.0 - 2.01.0 - 2.0Molten
 
Processing PropertiesMetricEnglishComments
Melt Temperature <= 204 °C<= 400 °F
 
Descriptive Properties
Coloroff-white
Suggested Application Temperature350°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PHBFULL000 / 316791

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.