MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

SABIC ULTEM™ Resin HU1100 Polyetherimide (PEI) (Asia)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change; biocompatible (ISO 10993 or USP Class VI); food contact compliant; Steam, Gamma, EtO, and E-beam sterilizable.

Features: Healthcare,High Stiffness,Steam, Gamma, EtO and E-beam sterilizable,Hydrolytic Stability,Chemical Resistance,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,High Heat Resistance,Good dimensional stability,Flame Retardant,Steam Sterilizable,Gamma Sterilizable,E-beam Sterilizable,Food Contact Acceptable,Biocompatible

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Moisture Absorption 0.0200 %0.0200 %Injection Molding
 0.700 %0.700 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.25 %1.25 %ISO 62-1
Viscosity 16 cP
@Load 5.00 kg,
Temperature 220 °C
16 cP
@Load 11.0 lb,
Temperature 428 °F
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
SABIC method
Melt Flow 8.8 g/10 min
@Load 6.60 kg,
Temperature 337 °C
8.8 g/10 min
@Load 14.6 lb,
Temperature 639 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 85.0 MPa12300 psi5 mm/min; ASTM D638
 85.0 MPa12300 psi5 mm/min; ISO 527
Tensile Strength, Yield 105 MPa15200 psi5 mm/min; ISO 527
 110 MPa16000 psi5 mm/min; ASTM D638
Elongation at Break 60 %60 %5 mm/min; ISO 527
 70 %70 %5 mm/min; ASTM D638
Elongation at Yield 6.0 %6.0 %5 mm/min; ISO 527
 7.0 %7.0 %5 mm/min; ASTM D638
Tensile Modulus 3.20 GPa464 ksi1 mm/min; ISO 527
 3.72 GPa540 ksi5 mm/min; ASTM D638
Flexural Strength 160 MPa23200 psiyield, 2 mm/min; ISO 178
 173 MPa25100 psiyld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 3.30 GPa479 ksi2 mm/min; ISO 178
 3.43 GPa497 ksi1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 37.0 J27.3 ft-lbASTM D256
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²80*10*4; ISO 180/1A
 6.00 kJ/m²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
80*10*4; ISO 180/1A
Charpy Impact, Notched 0.400 J/cm²1.90 ft-lb/in²Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 38.0 J28.0 ft-lbASTM D3763
 
Electrical PropertiesMetricEnglishComments
Arc Resistance 120 - 180 sec120 - 180 secASTM D495
Comparative Tracking Index 100 - 175 V100 - 175 VUL 746A
Hot Wire Ignition, HWI  30 - 60 sec
@Thickness >=0.750 mm
30 - 60 sec
@Thickness >=0.0295 in
UL 746A
 60 - 120 sec
@Thickness >=3.00 mm
60 - 120 sec
@Thickness >=0.118 in
UL 746A
High Amp Arc Ignition, HAI  0.00 - 15 arcs
@Thickness >=0.750 mm
0.00 - 15 arcs
@Thickness >=0.0295 in
UL 746A
 15 - 30 arcs
@Thickness >=3.00 mm
15 - 30 arcs
@Thickness >=0.118 in
UL 746A
High Voltage Arc-Tracking Rate, HVTR 25.4 - 80.0 mm/min1.00 - 3.15 in/minUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
CTE, linear, Transverse to Flow  55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ASTM E831
 55.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
30.6 µin/in-°F
@Temperature -40.0 - 104 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 188 °C370 °FFlatw 80*10*4 sp=64mm; ISO 75/Af
 198 °C
@Thickness 6.40 mm
388 °F
@Thickness 0.252 in
unannealed; ASTM D648
Vicat Softening Point 211 °C412 °FRate B/50; ASTM D1525
 211 °C412 °FRate B/50; ISO 306
 212 °C414 °FRate B/120; ISO 306
UL RTI, Electrical 170 °C338 °FUL 746B
UL RTI, Mechanical with Impact 170 °C338 °FUL 746B
UL RTI, Mechanical without Impact 170 °C338 °FUL 746B
Flammability, UL94  V-2
@Thickness >=0.400 mm
V-2
@Thickness >=0.0157 in
UL 94
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
UL 94
 5VA
@Thickness >=3.00 mm
5VA
@Thickness >=0.118 in
UL 94
 
Processing PropertiesMetricEnglishComments
Nozzle Temperature 345 - 400 °C653 - 752 °F
Zone 2 340 - 400 °C644 - 752 °F
Zone 3 345 - 400 °C653 - 752 °F
Melt Temperature 350 - 400 °C662 - 752 °FInjection Molding
Mold Temperature 135 - 165 °C275 - 329 °F
Drying Temperature 150 °C302 °FInjection Molding
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection Molding
 24.0 hour24.0 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa43.5 - 102 psi
Shot Size 40 - 60 %40 - 60 %
Vent Depth 0.00250 - 0.00760 cm0.000984 - 0.00299 in
Screw Speed 40 - 70 rpm40 - 70 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSABH82717 / 290664

USP Class VI Adhesives
USP Class VI Approved Adhesives for Medical Device Applications
Master Bond’s biocompatible adhesives are designed to meet the needs of medical device manufacturers. Compounds withstand various types of sterilization methods.

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.