MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Selenium, Se (alpha form)
Categories: Pure Element

Material Notes: CAS Number: 7782-49-2

Physical Form: Red Monoclinic Crystals

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 4.39 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 78.961995
Atomic Number 34
Critical Pressure 268.443 atm
Critical Temperature 1493 °C
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 84.73 J/g
Heat of Vaporization 1209 J/gAt Boiling Point
Specific Heat Capacity 0.2634 J/g-°CGas
 0.3217 J/g-°CCrystal
Melting Point 221 °C
Boiling Point 685 °C
Heat of Formation 0.000 kJ/molCrystal
 227.1 kJ/molGas
 
Descriptive Properties
SolubilityInsoluble in H2O and EtOH; Slightly Soluble in Ethyl Ether

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Selenium, Se (Gray Form)
Selenium, Se (Vitreous)
Copper (II) Sulfate Pentahydrate, CuSO4-5H2O
Copper (II) Sulfate, CuSO4
MV Labs CU1000 CuSO4·5H2O Copper(II) sulfate pentahydrate

AMESe01 / 5154

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.