MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Aremco-Seal™ 617 High Temperature Specialty Coatings Glass
Categories: Ceramic; Glass

Material Notes: Glass-filled adhesive/sealer for use with porous ceramics and refractories to 1500 ºF (816 ºC).

Key Words: Coatings
Vendors: Aremco offers a wide range of ceramic, glass and silicone based coatings for ceramic, glass and quartz materials used in heater and lighting applications to 2000°F (1093°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.45 g/cc1.45 g/cc
Solids Content 40.5 %40.5 %by volume
 51 %51 %by weight
Volatile Organic Compounds (VOC) Content 0.00 g/l0.00 g/l
Viscosity 1100 - 1500 cP1100 - 1500 cP
Thickness 25.4 microns1.00 milDry Film Thickness
 62.7 microns2.47 milWet Film Thickness
Storage Temperature 4.44 - 32.2 °C40.0 - 90.0 °F
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 816 °C1500 °FContinuous
 
Processing PropertiesMetricEnglishComments
Processing Temperature 10.0 - 32.2 °C50.0 - 90.0 °FApplication Temperature
Cure Time >= 30.0 min>= 0.500 hourAir Set prior to curing
 30.0 min
@Temperature 93.3 °C
0.500 hour
@Temperature 200 °F
+ 350°F, 60 min; + 1830°F, 1 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorClear
Theoretical Dry Film Coverage, ft²/gal650@ 1 mil
ThinnerWater

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAREM39 / 24303

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.