MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Teijin Panlite® B-8120R Carbon Fiber Reinforced Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Carbon Fiber Reinforced

Material Notes: CF 20% reinforced grade, meeting UL 94 V-2. It has excellent strength, stiffness, heat resistance and electric conductivity. Other features are low molding shrinkage and dimensional accuracy.

Applications:

  • Mechanical, electric and electronic components that need stiffness and strength
  • Mechanical, electric and electronic components that need extremely high dimensional accuracy.
  • Mechanical, electric and electronic components that need electric conductivity or antistatic property
  • Information provided by Teijin Chemicals Ltd.

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 1.29 g/cc0.0466 lb/in³ISO 1183
    Moisture Absorption 0.140 %
    @Temperature 23.0 °C,
    Time 86400 sec
    0.140 %
    @Temperature 73.4 °F,
    Time 24.0 hour
    ISO 62
    Linear Mold Shrinkage, Flow 0.00020 - 0.0020 cm/cm
    @Thickness 4.00 mm
    0.00020 - 0.0020 in/in
    @Thickness 0.157 in
    Teijin method
    Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm
    @Thickness 4.00 mm
    0.0030 - 0.0050 in/in
    @Thickness 0.157 in
    Teijin method
     
    Mechanical PropertiesMetricEnglishComments
    Tensile Strength at Break 130 MPa18900 psiISO 527-2/5
    Elongation at Break 1.5 %1.5 %ISO 527-2/5
    Tensile Modulus 13.6 GPa1970 ksiISO 527-2/1
    Flexural Strength 185 MPa26800 psi2.0 mm/min; ISO 178
    Flexural Modulus 12.0 GPa1740 ksi2.0 mm/min; ISO 178
    Charpy Impact Unnotched 2.50 J/cm²11.9 ft-lb/in²ISO 179
    Charpy Impact, Notched 0.700 J/cm²3.33 ft-lb/in²ISO 179
     
    Electrical PropertiesMetricEnglishComments
    Volume Resistivity 10 - 1000 ohm-cm10 - 1000 ohm-cmIEC 60093
    Surface Resistance 1.0 - 100 ohm1.0 - 100 ohmIEC 60093
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear, Parallel to Flow 20.0 µm/m-°C11.1 µin/in-°FISO 11359-2
    CTE, linear, Transverse to Flow 60.0 µm/m-°C33.3 µin/in-°FISO 11359-2
    Deflection Temperature at 0.46 MPa (66 psi) 149 °C300 °Funannealed; ISO 75-2/B
    Deflection Temperature at 1.8 MPa (264 psi) 147 °C297 °Funannealed; ISO 75-2/A
    Vicat Softening Point 152 °C306 °FISO 306/B50
    UL RTI, Electrical 80.0 °C
    @Thickness 1.50 mm
    176 °F
    @Thickness 0.0591 in
    UL 746
    UL RTI, Mechanical with Impact 80.0 °C
    @Thickness 1.50 mm
    176 °F
    @Thickness 0.0591 in
    UL 746
    UL RTI, Mechanical without Impact 80.0 °C
    @Thickness 1.50 mm
    176 °F
    @Thickness 0.0591 in
    UL 746
    Flammability, UL94  V-2
    @Thickness 0.750 mm
    V-2
    @Thickness 0.0295 in
     V-1
    @Thickness 3.00 mm
    V-1
    @Thickness 0.118 in

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Teijin Panlite® B-8110R Carbon Fiber Reinforced Polycarbonate Resin
    Overview of materials for Polycarbonate, Carbon Fiber Reinforced
    Teijin Panlite® B-8130R Carbon Fiber Reinforced Polycarbonate Resin
    RTP Company RTP 382 Polycarbonate (PC), Carbon Fiber
    RTP Company RTP 381 Polycarbonate (PC), Carbon Fiber

    PTEIJ21 / 69710

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.