MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Trinseo CALIBRE™ 301 HMR FC030003 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Molded

Material Notes: CALIBRE™ 301 HMR FC030003 Polycarbonate resin offers exceptional impact resistance, heat distortion resistance, and optical clarity. CALIBRE™ 301 HMR also has a mold release package designed to improve processing larger more complex injection molded parts.

Applications:

  • Small & Large appliances

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183/A
Water Absorption 0.15 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 0.32 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 in/inISO 294-4
Melt Flow 19 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73ASTM D785
Hardness, Rockwell R 118ASTM D785
Tensile Strength at Break 71.0 MPaISO 527-2/50
Tensile Strength, Yield 60.0 MPaISO 527-2/50
Elongation at Break 150 %ISO 527-2/50
Elongation at Yield 6.0 %ISO 527-2/50
Tensile Modulus 2300 MPaISO 527-2/50
Flexural Strength 97.0 MPa2.0 mm/min; ISO 178
Flexural Modulus 2400 MPa2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 83.0 kJ/m²ISO 180/A
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
Abrasion 45[%], Taber; ASTM D1044
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.0
@Frequency 60 Hz
IEC 60250
 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 17.0 kV/mmIEC 60243-1
Dissipation Factor 0.0010
@Frequency 50 Hz
IEC 60250
 0.0020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 250 V
@Thickness 2.00 mm
Solution A; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 70.0 µm/m-°CASTM D696
Hot Ball Pressure Test >= 125 °CIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 143 °CAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 124 °CUnannealed; ISO 75-2/A
 140 °CAnnealed; ISO 75-2/A
Vicat Softening Point 148 °CISO 306/B50
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489
Haze <= 1.0 %ASTM D1003
Transmission, Visible 89 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
MRC Polymers NAXELL™ PC110-919 General Purpose Polycarbonate, Medium High MFR
MRC Polymers NAXELL PC100H High MFR Polycarbonate
Clariant Renol PCSP0006WT-181 Polycarbonate, Laser Markable
Clariant Renol PCSP0006GY-371 Polycarbonate, Laser Markable
Avient Edgetek® PC-40GF-000 FR MR Polycarbonate (PC), Glass Filled

PTRINS9014 / 197538

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.