MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Marco Polo MARPOL mLLF 801-CSB Linear Low Density Polyethylene - Metallocene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: MARPOL® mLLF 801-CSB is a clarity grade ethylene-hexene copolymer produced with metallocene single site catalyst. This grade has excellent clarity and outstanding tensile, impact, puncture, resistance and low temperature properties. mLLF 801-CSB contains slip and antiblock making it suitable for formulations which require good openability and a low friction coefficient.

Recommended Applications: Clarity packaging, film for frozen food, high speed form-fill seal packaging, heavy duty packaging, bag in boxes, trash bags, liners.

Additives: Antiblock – 4500 ppm, Slip – 1000 ppm.

Information provided by Marco Polo International, LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D1505
Melt Flow 1.3 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.3 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Antiblock Level 4500 ppm4500 ppm
Slip Level 1000 ppm1000 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.4 MPa1800 psiASTM D882
Film Tensile Strength at Yield, TD 9.65 MPa1400 psiASTM D882
Film Elongation at Break, MD 450 %450 %ASTM D882
Film Elongation at Break, TD 500 %500 %ASTM D882
Flexural Modulus, 1% Secant 21000 MPa3.05e+6 psiMD; ASTM D882
 22000 MPa3.19e+6 psiTD; ASTM D882
Elmendorf Tear Strength MD 250 g250 gASTM D1922
Elmendorf Tear Strength TD 500 g500 gASTM D1922
Dart Drop Test 700 g1.54 lbASTM D1709A
Film Tensile Strength at Break, MD 51.7 MPa7500 psiASTM D882
Film Tensile Strength at Break, TD 44.5 MPa6450 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 120 °C248 °FASTM D3418
 
Optical PropertiesMetricEnglishComments
Haze 8.5 %8.5 %ASTM D1003
Gloss 105 %105 %60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMARCO160 / 283757

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.