MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Platinum, Pt, Thermocouple Quality, Annealed
Categories: Metal; Nonferrous Metal; Precious Metal; Platinum Alloy; Pure Element

Material Notes: Thermocouple Quality is 99.99% pure.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 21.45 g/cc
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 195.0781995
Atomic Number 78
Thermal Neutron Cross Section 9.0 barns/atom
X-ray Absorption Edge 0.15817 ÅK
 0.89405 ÅLI
 0.93484 ÅLII
 1.07306 ÅLIII
Electrode Potential 1.2 V
Electronegativity 2.2Pauling
Ionic Radius 0.650 ÅCrystal Ionic Radius for Valence +4
 0.800 ÅCrystal Ionic Radius for Valence +2
Electrochemical Equivalent 1.816 g/A/h
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 40
Tensile Strength, Ultimate 143 MPa
Elongation at Break 35 %in 50 mm
Tensile Modulus 171 GPastatic
Poissons Ratio 0.39
Shear Modulus 62.0 GPaCalculated value
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000106 ohm-cmTemperature Coefficient of resistivity is 0.0039/K.
Magnetic Susceptibility 0.0000011cgs/g
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 113 J/g
Heat of Vaporization 2407 J/g
CTE, linear 9.10 µm/m-°C
@Temperature 20.0 °C
Specific Heat Capacity 0.134 J/g-°C
Thermal Conductivity 69.1 W/m-K
Melting Point 1769 °C
Boiling Point 3825 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.30650 nm
 0.152
@Temperature 1000 °C
Total Hemispherical
Reflection Coefficient, Visible (0-1) 0.70bulk Pt; 589 nm
 
Component Elements PropertiesOriginal ValueComments
Platinum, Pt 99.99 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Silicon, Si
Platinum, Pt, CP Grade, Annealed
Platinum, Pt, CP Grade, Hard Drawn - 50% Cold Worked
Pt-10% Rh Alloy, Annealed
Aluminum, Al

AMEPt03 / 87

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.