  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Solvay Chemicals Allyl chloride High purity 3-chloropropene
Categories: Fluid

Material Notes: Allyl chloride is mainly used in the manufacture of epichlorohydrin. It is also used in the production of allylic ethers, esters, silanes and quaternary ammonium derivatives.

EINECS Number: 203-457-6/CAS Number: 107-05-1/UN number: 1100

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density  0.7911 g/cc
@Pressure 0.7726 MPa,
Temperature 120 °C
0.02858 lb/in³
@Pressure 112.1 psi,
Temperature 248 °F
 0.8084 g/cc
@Pressure 0.6201 MPa,
Temperature 110 °C
0.02921 lb/in³
@Pressure 89.94 psi,
Temperature 230 °F
 0.825 g/cc
@Pressure 0.4912 MPa,
Temperature 100 °C
0.0298 lb/in³
@Pressure 71.24 psi,
Temperature 212 °F
 0.8411 g/cc
@Pressure 0.3835 MPa,
Temperature 90.0 °C
0.03039 lb/in³
@Pressure 55.62 psi,
Temperature 194 °F
 0.8565 g/cc
@Pressure 0.2947 MPa,
Temperature 80.0 °C
0.03094 lb/in³
@Pressure 42.74 psi,
Temperature 176 °F
 0.8714 g/cc
@Pressure 0.2226 MPa,
Temperature 70.0 °C
0.03148 lb/in³
@Pressure 32.29 psi,
Temperature 158 °F
 0.8859 g/cc
@Pressure 0.1649 MPa,
Temperature 60.0 °C
0.03201 lb/in³
@Pressure 23.92 psi,
Temperature 140 °F
 0.8999 g/cc
@Pressure 0.1196 MPa,
Temperature 50.0 °C
0.03251 lb/in³
@Pressure 17.35 psi,
Temperature 122 °F
 0.9136 g/cc
@Pressure 0.0848 MPa,
Temperature 40.0 °C
0.03301 lb/in³
@Pressure 12.3 psi,
Temperature 104 °F
 0.9203 g/cc
@Pressure 0.0707 MPa,
Temperature 35.0 °C
0.03325 lb/in³
@Pressure 10.3 psi,
Temperature 95.0 °F
 0.9269 g/cc
@Pressure 0.0585 MPa,
Temperature 30.0 °C
0.03349 lb/in³
@Pressure 8.48 psi,
Temperature 86.0 °F
 0.9334 g/cc
@Pressure 0.0481 MPa,
Temperature 25.0 °C
0.03372 lb/in³
@Pressure 6.98 psi,
Temperature 77.0 °F
 0.9398 g/cc
@Pressure 0.0392 MPa,
Temperature 20.0 °C
0.03395 lb/in³
@Pressure 5.69 psi,
Temperature 68.0 °F
 0.9462 g/cc
@Pressure 0.0317 MPa,
Temperature 15.0 °C
0.03418 lb/in³
@Pressure 4.60 psi,
Temperature 59.0 °F
 0.9525 g/cc
@Pressure 0.0254 MPa,
Temperature 10.0 °C
0.03441 lb/in³
@Pressure 3.68 psi,
Temperature 50.0 °F
 0.9587 g/cc
@Pressure 0.0202 MPa,
Temperature 5.00 °C
0.03464 lb/in³
@Pressure 2.93 psi,
Temperature 41.0 °F
 0.9648 g/cc
@Pressure 0.0159 MPa,
Temperature 0.000 °C
0.03486 lb/in³
@Pressure 2.31 psi,
Temperature 32.0 °F
 0.9709 g/cc
@Pressure 0.0124 MPa,
Temperature -5.00 °C
0.03508 lb/in³
@Pressure 1.80 psi,
Temperature 23.0 °F
 0.9769 g/cc
@Pressure 0.00950 MPa,
Temperature -10.0 °C
0.03529 lb/in³
@Pressure 1.38 psi,
Temperature 14.0 °F
 0.9828 g/cc
@Pressure 0.00720 MPa,
Temperature -15.0 °C
0.03551 lb/in³
@Pressure 1.04 psi,
Temperature 5.00 °F
 0.9887 g/cc
@Pressure 0.00540 MPa,
Temperature -20.0 °C
0.03572 lb/in³
@Pressure 0.783 psi,
Temperature -4.00 °F
 1.0003 g/cc
@Pressure 0.00290 MPa,
Temperature -30.0 °C
0.036138 lb/in³
@Pressure 0.421 psi,
Temperature -22.0 °F
Solubility in Water 0.36 %0.36 %
Viscosity 0.34 cP0.34 cP
Molecular Weight 76.53 g/mol76.53 g/mol
Vapor Pressure 0.400 bar300 torr
Surface Tension 0.023 dynes/cm0.023 dynes/cm
 
Chemical PropertiesMetricEnglishComments
Critical Pressure 48.0 bar36000 torr
Critical Temperature 241 °C466 °F
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  1.013
@Temperature 19.0 °C
1.013
@Temperature 66.2 °F
vapor
 8.2
@Temperature 20.0 °C
8.2
@Temperature 68.0 °F
liquid
 
Thermal PropertiesMetricEnglishComments
Specific Heat Capacity 0.950 J/g-°C0.227 BTU/lb-°Fvapor
 1.50 J/g-°C0.359 BTU/lb-°Fliquid
Melting Point -135 °C-211 °FFreezing Point
Boiling Point 43.0 °C109 °FAzeotrope with water
 45.0 °C
@Pressure 1.013 MPa
113 °F
@Pressure 146.9 psi
Decomposition Temperature >= 80.0 °C>= 176 °F
Flash Point -27.0 °C-16.6 °FTAG closed cup
Ignition Temperature >= 392 °C>= 738 °FAutoignition
 
Descriptive Properties
AppearanceClear liquid, free from visible matter or particles
Coefficient of volume expansion0.0014K-1
Combustion heat24 kJ/g
Composition<100 mg/kgWater, ASTM D3401, ASTM E1064
 >99%Allyl Chloride - assay
 0.5-90.9 g/kgStabilizer
 22 g/kgAzeotrope with water, content
Flammability limits3.3-11.2%
Latent heat of evaporation0.37 kJ/g45°C
Partition coefficient P2.1 Log P o/wn-octanol.water
Solubility of water in organic0.8 g/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Acrylic, General Purpose, Molded
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Overview of materials for Epoxy Adhesive
Overview of materials for Nylon 6, Unreinforced
Overview of materials for Nylon 66/6

WSOLV132 / 147781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.