MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott SFL57 847236.355, Optical Glass
Categories: Ceramic; Glass; Optical

Material Notes:

Information provided by SCHOTT.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.55 g/cc0.128 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 1.31.3
Alkali Class, AR 1.01.0
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 580580HK (0.1/20)
Modulus of Elasticity 97.0 GPa14100 ksi
Poissons Ratio 0.2160.216
Shear Modulus 39.9 GPa5790 ksiCalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.70 µm/m-°C
@Temperature -30.0 - 70.0 °C
4.83 µin/in-°F
@Temperature -22.0 - 158 °F
 10.0 µm/m-°C
@Temperature 20.0 - 300 °C
5.56 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.670 J/g-°C0.160 BTU/lb-°F
Thermal Conductivity 0.997 W/m-K6.92 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 598 °C1110 °F
Softening Point 700 °C1290 °Fviscosity of 107.6 cP
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.784
@Wavelength 2325.45 nm
1.784
@Wavelength 2325.45 nm
 1.791
@Wavelength 1970.1 nm
1.791
@Wavelength 1970.1 nm
 1.799
@Wavelength 1529.6 nm
1.799
@Wavelength 1529.6 nm
 1.811
@Wavelength 1060 nm
1.811
@Wavelength 1060 nm
 1.812
@Wavelength 1014 nm
1.812
@Wavelength 1014 nm
 1.82
@Wavelength 852.1 nm
1.82
@Wavelength 852.1 nm
 1.83
@Wavelength 706.5 nm
1.83
@Wavelength 706.5 nm
 1.836
@Wavelength 656.3 nm
1.836
@Wavelength 656.3 nm
 1.838
@Wavelength 643.8 nm
1.838
@Wavelength 643.8 nm
 1.839
@Wavelength 632.8 nm
1.839
@Wavelength 632.8 nm
 1.846
@Wavelength 587.6 nm
1.846
@Wavelength 587.6 nm
 1.846
@Wavelength 589.3 nm
1.846
@Wavelength 589.3 nm
 1.855
@Wavelength 546.1 nm
1.855
@Wavelength 546.1 nm
 1.872
@Wavelength 486.1 nm
1.872
@Wavelength 486.1 nm
 1.874
@Wavelength 480 nm
1.874
@Wavelength 480 nm
 1.894
@Wavelength 435.8 nm
1.894
@Wavelength 435.8 nm
 1.914
@Wavelength 404.7 nm
1.914
@Wavelength 404.7 nm
Abbe Number 23.4323.43ve
 23.6223.62vd
Optical Dispersion 0.0358410.035841nf - nc
 0.0364890.036489nf' - nc'
Transmission, Visible  52 %
@Thickness 25.0 mm,
Wavelength 420 nm
52 %
@Thickness 0.984 in,
Wavelength 420 nm
 67 %
@Thickness 25.0 mm,
Wavelength 436 nm
67 %
@Thickness 0.984 in,
Wavelength 436 nm
 77 %
@Thickness 10.0 mm,
Wavelength 420 nm
77 %
@Thickness 0.394 in,
Wavelength 420 nm
 80 %
@Thickness 25.0 mm,
Wavelength 460 nm
80 %
@Thickness 0.984 in,
Wavelength 460 nm
 85.2 %
@Thickness 10.0 mm,
Wavelength 436 nm
85.2 %
@Thickness 0.394 in,
Wavelength 436 nm
 89 %
@Thickness 25.0 mm,
Wavelength 500 nm
89 %
@Thickness 0.984 in,
Wavelength 500 nm
 91.5 %
@Thickness 10.0 mm,
Wavelength 460 nm
91.5 %
@Thickness 0.394 in,
Wavelength 460 nm
 95.4 %
@Thickness 10.0 mm,
Wavelength 500 nm
95.4 %
@Thickness 0.394 in,
Wavelength 500 nm
 95.5 %
@Thickness 25.0 mm,
Wavelength 546 nm
95.5 %
@Thickness 0.984 in,
Wavelength 546 nm
 96.9 %
@Thickness 25.0 mm,
Wavelength 660 nm
96.9 %
@Thickness 0.984 in,
Wavelength 660 nm
 97.1 %
@Thickness 25.0 mm,
Wavelength 620 nm
97.1 %
@Thickness 0.984 in,
Wavelength 620 nm
 97.1 %
@Thickness 25.0 mm,
Wavelength 580 nm
97.1 %
@Thickness 0.984 in,
Wavelength 580 nm
 97.6 %
@Thickness 25.0 mm,
Wavelength 700 nm
97.6 %
@Thickness 0.984 in,
Wavelength 700 nm
 98.2 %
@Thickness 10.0 mm,
Wavelength 546 nm
98.2 %
@Thickness 0.394 in,
Wavelength 546 nm
 98.7 %
@Thickness 10.0 mm,
Wavelength 660 nm
98.7 %
@Thickness 0.394 in,
Wavelength 660 nm
 98.8 %
@Thickness 10.0 mm,
Wavelength 620 nm
98.8 %
@Thickness 0.394 in,
Wavelength 620 nm
 98.8 %
@Thickness 10.0 mm,
Wavelength 580 nm
98.8 %
@Thickness 0.394 in,
Wavelength 580 nm
 99 %
@Thickness 10.0 mm,
Wavelength 700 nm
99 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  73 %
@Thickness 25.0 mm,
Wavelength 2500 nm
73 %
@Thickness 0.984 in,
Wavelength 2500 nm
 79 %
@Thickness 25.0 mm,
Wavelength 2325 nm
79 %
@Thickness 0.984 in,
Wavelength 2325 nm
 88.2 %
@Thickness 10.0 mm,
Wavelength 2500 nm
88.2 %
@Thickness 0.394 in,
Wavelength 2500 nm
 91 %
@Thickness 10.0 mm,
Wavelength 2325 nm
91 %
@Thickness 0.394 in,
Wavelength 2325 nm
 96 %
@Thickness 25.0 mm,
Wavelength 1970 nm
96 %
@Thickness 0.984 in,
Wavelength 1970 nm
 98.4 %
@Thickness 10.0 mm,
Wavelength 1970 nm
98.4 %
@Thickness 0.394 in,
Wavelength 1970 nm
 99 %
@Thickness 25.0 mm,
Wavelength 1530 nm
99 %
@Thickness 0.984 in,
Wavelength 1530 nm
 99.1 %
@Thickness 25.0 mm,
Wavelength 1060 nm
99.1 %
@Thickness 0.984 in,
Wavelength 1060 nm
 99.6 %
@Thickness 10.0 mm,
Wavelength 1060 nm
99.6 %
@Thickness 0.394 in,
Wavelength 1060 nm
 99.6 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.6 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  3.0 %
@Thickness 25.0 mm,
Wavelength 390 nm
3.0 %
@Thickness 0.984 in,
Wavelength 390 nm
 5.0 %
@Thickness 10.0 mm,
Wavelength 380 nm
5.0 %
@Thickness 0.394 in,
Wavelength 380 nm
 20 %
@Thickness 25.0 mm,
Wavelength 400 nm
20 %
@Thickness 0.984 in,
Wavelength 400 nm
 26 %
@Thickness 10.0 mm,
Wavelength 390 nm
26 %
@Thickness 0.394 in,
Wavelength 390 nm
 29 %
@Thickness 25.0 mm,
Wavelength 405 nm
29 %
@Thickness 0.984 in,
Wavelength 405 nm
 52.5 %
@Thickness 10.0 mm,
Wavelength 400 nm
52.5 %
@Thickness 0.394 in,
Wavelength 400 nm
 60.9 %
@Thickness 10.0 mm,
Wavelength 405 nm
60.9 %
@Thickness 0.394 in,
Wavelength 405 nm
 
Descriptive Properties
Climatic resistance1
Grindability3ISO 12844
Phosphate resistance1.3
Stress optical coefficient2.73[10-6mm2/N]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Titanium Grade 2
Schott N-PSK53 620635.360, Optical Glass

CSGT9877 / 183130

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.