MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chesterton 710 Anti-Seize Compound
Categories: Fluid; Lubricant

Material Notes: Description: Chesterton® 710 Anti-Seize Compound is an anti-seize compound and assembly lubricant combining the high temperature, extreme pressure, and corrosion resistant properties of colloidal copper, aluminum and graphite in an oil based suspension that will not burn, scrape or wash-off. The product seals and protects metal parts under extreme conditions by providing an ultra-thin coating of copper particles. The fine colloidal particles coat and separate metal parts, thus retarding pitting from galvanic action between dissimilar metals and the micro welding that could occur if asperities in the metal were not kept apart. Because 710 Anti-Seize Compound has a balanced coefficient of friction, threads are not stretched and more accurate load values are possible during assembly. The product saves threads and parts for reuse by preventing falling damage and breakage during opening. Chesterton 710 Anti-Seize Compound meets MIL-A-907D and is on the U.S. Navy qualified products list QPL-907. It is NSF registered for use in federally inspected meat and poultry plants.

Applications: Use on steel, stainless steel, iron, copper, brass, titanium, etc. Do not use on oxygen systems or in presence of acetylene. Listed below are several specific applications:Automotive Industry-For metal gaskets, studs in cylinder heads, valve guides, u-bolts, etc Diesel engine bolts, flanges, fittingsFoundry-For coating molds before pouring in metal to prevent sticking and breakageUtilities-Underground and high pressure valves, fittings and shut-off valvesMachine Shops-Solder iron release, torque wrench accessory, cranes, conveyers, etc. Plumbing-For high pressure, threaded or flanged jointsPumps-On flanges, bolts and fittings for high temperature applicationsLift Trucks-Lubrication and corrosion protection for bearings, sprockets, chains and wear surfacesFurnaces-On heat-treat furnaces and foundry operations to prevent seizure of fasteners on parts due to high temperatures.
On stainless steel at higher temperatures and on aluminum, it is recommended to use Chesterton® 785 Nickel Anti-Seize Compound or Chesterton® 785 Parting Lubricant for the rubber molding industry, for salt water applications, and in aggressive acid or alkaline environments.

Information provided by Chesterton

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Particle Size 4.0 - 7.0 µm4.0 - 7.0 µm
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.0800.080ASTM D2266, DIN 51 350
 0.200.20"K" Factor; ASTM D2266, DIN 51 350
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1100 °C2010 °F
Flash Point 85.0 °C185 °F
Dropping Point >= 204 °C>= 399 °FASTM D566, ISO 2176
 
Descriptive Properties
ColorCopper
Consistency1NLGI
 Soft Paste
Extreme Pressure Capability116564 psiASTM D2788, DIN 51 350

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Sinotek Materials Tungsten Disulfide (WS2) Powder, High-Purity
Okulen® 2000 PE-UHMW, DryRun
Nylacast Nylube Cast Nylon 6, Lubricated (Blended Solid and Liquid Lubricant)
Chesterton 785 Parting Lubricant

PPTCHS090 / 138202

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.