MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

3M Novec™ 71IPA Engineered Fluid
Categories: Fluid

Material Notes: 3M™ Novec™ 71IPA Engineered Fluid is ideal for light cleaning and degreasing tasks. 3M™ Novec™ 71IPA has essentially constant vapor and liquid composition at its boiling point. Excellent replacement for IPA where nonflammability is important.

Feature and Benefits:

  • Non-flammable
  • Non-conductive
  • Low toxicity
  • Low Global Warming Potential (GWP)
  • Zero ozone depletion potential
  • Low surface tension penetrates tight spaces for improved cleaning

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.52 g/cc0.0549 lb/in³Liquid
Vapor Pressure 0.269 bar202 torr
Surface Tension 13.6 dynes/cm13.6 dynes/cm
 
Thermal PropertiesMetricEnglishComments
Heat of Vaporization 125.6 J/g54.03 BTU/lb
Boiling Point 61.0 °C142 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Novec™ 7100DL Engineered Fluid
3M Novec™ 7100 Engineered Fluid
3M Novec™ 7000 Engineered Fluid
3M Novec™ 649 Engineered Fluid
3M Novec™ 71DA Engineered Fluid

PMM33108 / 167855

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.