MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Avient Therma-Tech™ SFC-5000 TC Polyphenylene Sulfide (PPS)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of thermoplastics. These materials provide the benefits of proprietary conductive additive technologies and the performance of select engineering thermoplastic resins. Therma-Tech compounds have been shown to improve thermal conductivity up to 100-times that of conventional plastics and can be used in a wide range of thermal management applications.

Description/Features:

  • PPS (Polyphenylenesulfide)
  • Thermally Conductive
  • Electrically Conductive

Applications:

  • Enclosures
  • Heat Sinks
  • Motor components

Processing Method: Injection Molding

Information provided by PolyOne Corporation

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 g/ccASTM D792
Water Absorption 0.030 %
@Thickness 3.17 mm
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 9000 psiType 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 0.30 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 3.20e+6 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 14500 psiASTM D790
Flexural Modulus 2.80e+6 psiASTM D790
Izod Impact, Notched 0.500 ft-lb/in
@Thickness 6.35 mm,
Temperature 23.0 °C
Method A, Injection Molded; ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 100 - 1000 ohm-cmASTM D257
Surface Resistivity per Square 10 - 100 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 6.94 - 13.9 BTU-in/hr-ft²-°FASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 530 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 500 °FUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Melt Temperature 600 - 625 °FMolding
Mold Temperature 250 - 300 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Avient Therma-Tech™ SF-5000C TC Polyphenylene Sulfide (PPS)
Avient Therma-Tech™ SF-6000 TC Polyphenylene Sulfide (PPS)
Avient OnForce™ LFT LF9200-5001 RS Natural Polyphenylene Sulfide (PPS)
Avient LubriOne™ SF-30GF/15T Polyphenylene Sulfide (PPS)
Avient LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS)

PH1PO3366e / 45041

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.