MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Wellman Wellamid® MRGF25/15 42H-BK167A Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Glass/Mineral Reinforced

Material Notes: GM 167A Black color match

All information provided by Wellman Engineered Resins.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.50 g/cc0.0542 lb/in³ISO 1183-87
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inDIS 294-4
Linear Mold Shrinkage, Transverse 0.0080 - 0.012 cm/cm0.0080 - 0.012 in/inDIS 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 115 MPa16700 psiISO 527-93
Elongation at Break 2.0 %2.0 %ISO 527-93
Flexural Strength 170 MPa24700 psiISO 178-93
Flexural Modulus 10.1 GPa1460 ksiISO 178-93
Izod Impact, Notched (ISO) 4.00 kJ/m²1.90 ft-lb/in²ISO 180-93
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-93

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wellman Wellamid® MRGF25/15 42H-WBK Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced, Weatherable Grade
Wellman Wellamid® MRGF30/10 42H-NBK1 Nylon 6, 30% Mineral and 10% Glass Reinforced
Wellman Wellamid® MRGF30/10 42H-GY1 Nylon 6, 30% Mineral and 10% Glass Reinforced
Wellman Wellamid® MRGF25/15 42H-NBK1 40% Mineral/Glass Fiber Reinforced Nylon 6
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced

PWEL00122 / 88042

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.