MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco Ceramabond™ 685  (discontinued **)
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Bonds porous ceramics to plated and galvanized metals.

Key Words: adhesives, ceramic, ceramics, bonding, bond, adhesive
Vendors: Aremco’s ceramic and graphite adhesives are ideal for bonding, potting and sealing probes, sensors, halogen lamps, igniters, power resistors, cartridge heaters, filters, fiberoptics, honeycombs, and graphite structures to 3200°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 1.00e+9 ohm-cm1.00e+9 ohm-cmat RT
 1e+05
@Temperature 540 °C
1e+05
@Temperature 1000 °F
Dielectric Strength  5.90 kV/mm
@Temperature 538 °C
150 kV/in
@Temperature 1000 °F
 8.00 kV/mm
@Temperature 22.2 °C
203 kV/in
@Temperature 72.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 10.8 µm/m-°C
@Temperature 20.0 °C
6.00 µin/in-°F
@Temperature 68.0 °F
Maximum Service Temperature, Air 1010 °C1850 °F
 
Descriptive Properties
ColorTan

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Ceramabind™ 542 High Temperature Inorganic Binder
Aremco Ceramabind™ 642 High Temperature Inorganic Binder
Aremco Ceramabind™ 642-A High Temperature Inorganic Binder
Aremco Ceramabind™ 643-1 High Temperature Inorganic Binder
Aremco Ceramabind™ 643-2 High Temperature Inorganic Binder

ZCAR022 / 503

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.