  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Ceramacast™ 515 High Temperature Potting & Casting Aluminum Oxide
Categories: Ceramic; Oxide; Silicon Oxide; Potting/Casting Ceramic

Material Notes: Fine Grain, High Strength Potting Compound. Binder is K2O-SiO2

Cure:
Step 1. Dry for 16–24 hours at room temperature.
Step 2. Bake at 200ºF for 1–4 hours.
Step 3. Bake at 250ºF for 1–4 hours.
Step 4. Bake at 350ºF for 1 hour.
Step 5. Final cure at 500ºF for 1 hour.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.44 g/cc
Porosity <= 2.0 %
pH 11 - 12
Viscosity 10000 cPMixed
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 11000 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+9 ohm-cm
Dielectric Strength 250 V/mil
 
Thermal PropertiesOriginal ValueComments
CTE, linear 4.50 µin/in-°F
@Temperature 20.0 °C
Maximum Service Temperature, Air 3000 °F
Shrinkage <= 1 %
@Temperature 538 °C
 
Processing PropertiesOriginal ValueComments
Dry Time 20 - 24.0 hourAir dry prior to cure
Cure Time 5.00 - 7.00 hoursee notes
Pot Life 120 - 180 min
Shelf Life 12.0 Month
 
Descriptive Properties
Acid ResistanceGoodattacked by HF
Alkali ResistanceGood
BinderK2-SiO2
ColorWhite
Mix Ratio100:12-14powder:water
Moisture ResistanceGood

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CAREM46m / 256033

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.