MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Pyrotek Pyrocast ICL Castable Refractory
Categories: Ceramic; Oxide; Silicon Oxide

Material Notes: Pyrocast ICL was developed exclusively for the induction furnace market as a coil lining refractory. This silica and alumina based material displays high strength and excellent thermal shock resistance.

Applications

  • Induction coil lining
  • Boiler preheater lining
  • Component linings

Advantages

  • Excellent window for induction energy
  • Extremely stable
  • Thermal shock resistant
  • Minimum maintenance
  • Resilient to cracking
  • Fewest shorts
  • Long-life coil lining

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.89 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.0100 GPa
Compressive Strength 41.0 MPa
 
Thermal PropertiesOriginal ValueComments
CTE, linear 0.250 µm/m-°C
@Temperature <=1010 °C
Thermal Conductivity 0.620 W/m-K
@Temperature 295 °C
 0.690 W/m-K
@Temperature 540 °C
 0.820 W/m-K
@Temperature 815 °C
Maximum Service Temperature, Air 1650 °C
Shrinkage 0.20 %
@Temperature 1090 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek Pyrocast AR PLUS Castable Refractory
Pyrotek Pyrocast AR70 Low-Density Refractory Castable
Pyrotek Pyrocast AR-S Castable Refractory
Pyrotek Pyrocast HD Castable Refractory
Pyrotek Pyrocast PCR Abrasion-Resistant Refractory Castable

CPYRO143 / 1864

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.