MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Momentive Performance Materials Silopren LSR 3486 50 TP4268 Liquid Silicone Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber; Liquid Silicone Rubber (LSR)

Material Notes: Silopren LSR 3486/50 is a two-component liquid silicone rubber for injection molding processes. This material is an excellent candidate to consider for the manufacture of elastomeric articles requiring self-lubricating properties. The self-lubricating effect is achieved by a fluid which exudes out of the vulcanizate over an extended period of time. It typically starts between a few hours and one day after vulcanization. Silopren LSR 3486/50 liquid silicone rubber shows a low compression set after vulcanization without post-curing. Vulcanizates consisting of Silopren LSR 3486/50 liquid silicone rubber are typically distinguished by the following properties: low compression set without post-cure, self-lubricating properties, low viscosity, fast cure, high thermal stability, outstanding resistance to aging, easy to color. Because of the outstanding properties, Silopren LSR 3486/50 liquid silicone rubber is an excellent candidate to consider for use in wire harness applications for the following elastomeric articles: cable seals, grommets, gaskets, plug seals.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.12 g/cc0.0405 lb/in³DIN 53 479 A
Viscosity 360000 cP360000 cPUncured. B-part. gamma=10s-1 at 20°C.; DIN 53018
 480000 cP480000 cPUncured. A- part. gamma=10s-1 at 20°C.; DIN 53018
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 5151DIN 53 505
Tensile Strength 8.10 MPa1170 psiDIN 53 504 S2
Elongation at Break 540 %540 %DIN 53 504 S2
Tear Strength 44.0 kN/m251 pliASTM D 624
Compression Set 25 %25 %DIN ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 175 °C
@Time 601 sec
347 °F
@Time 0.167 hour
Vulcanization as Tested; Die B
Pot Life 4320 min
@Temperature 20.0 °C
4320 min
@Temperature 68.0 °F
Closed vessel
 
Descriptive Properties
ColorWhitishUncured. A-part.
 WhitishUncured. B-part
Fluid Content (%)4Uncured. A-part
 4Uncured. B-part
Mix Ratio1:1 A:BAs Tested

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMOMEN9989 / 265804

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.