MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

ITW Devcon® DFense Blok™ Quick Patch Wear-Resistant Epoxy Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: Alumina ceramic bead-filled epoxy system with a very fast cure speed, allowing for emergency patching of processing equipment. Provides wear and abrasion resistance for extended service life. Uses: Patch holes, leaks and cracks in all types of processing equipment such as: scrubbers, ash handling systems, pipe elbows, screens, chutes, recontour chippers, bins, hoppers, bunkers, separators, digester tables, exhausters, launderers, housing fans, crushers and breakers. Features: Eliminates downtime, Exceptionally fast cure for emergency patching, Applies to vertical and overhead surfaces, Easy to mix, Ceramic beads for wear resistance.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.86 g/cc1.86 g/ccCured
Solids Content 100 %100 %Uncured
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 8484
Flexural Strength 33.6 MPa4880 psiASTM D790
Compressive Strength 42.51 MPa6166 psiASTM D695
Adhesive Bond Strength 17.20 MPa2495 psiAdhesive Tensile Shear; ASTM D1002
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5151ASTM D150
 
Thermal PropertiesMetricEnglishComments
CTE, linear 55.8 µm/m-°C31.0 µin/in-°FASTM D696
Maximum Service Temperature, Air 93.3 °C200 °FTemperature Resistance - Dry
Shrinkage 0.10 %0.10 %Linear During cure; ASTM D2566
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 24.0 °C
0.500 hour
@Temperature 75.2 °F
Functional cure
 360 min
@Temperature 24.0 °C
6.00 hour
@Temperature 75.2 °F
 10100 min
@Temperature 24.0 °C
168 hour
@Temperature 75.2 °F
As Tested
Pot Life 4.00 min
@Temperature 23.9 °C
4.00 min
@Temperature 75.0 °F
 
Descriptive Properties
Chemical/Solvent Resistance1,1,1-Trichloroethane: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Ammonia: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Gasoline (Unleaded): very good30 day immersion at 75°F. Sample cured 7 days at RT
 Hydrochloric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Methanol: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Methyl Ethyl Ketone: poor30 day immersion at 75°F. Sample cured 7 days at RT
 Sodium Hydroxide 50%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Sulfuric Acid 10%: fair30 day immersion at 75°F. Sample cured 7 days at RT
 Trisodium Phosphate: fair30 day immersion at 75°F. Sample cured 7 days at RT
ColorGrayCured
Coverage60 sq. in/lbUncured at 1/4"
Mix Ratio by volume1:1
Mix Ratio by weight1:1
Recoat Time20 to 30 minutes
Specific Volume (in.³/lb)14.89Cured
ViscosityNon-sag putty Mixed

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PITWD9174 / 239684

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.