System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Fluorseals PTFE 15% graphite filled
Categories:
Polymer
;
Thermoplastic
;
Fluoropolymer
;
Polytetrafluoroethylene (PTFE)
Material Notes:
Improved thermal conductivity and coefficient of friction.
Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
2.17
g/cc
ASTM 1457-62 T
Deformation
7.0 %
14 MPa, 100 h, 23°C; ASTM D621-59
Mechanical Properties
Original Value
Comments
Ball Indentation Hardness
32.0
MPa
ASTM 1457-62 T
Tensile Strength at Break
14.0
MPa
ASTM 1457-62 T
Elongation at Break
160 %
ASTM 1457-62 T
Coefficient of Friction, Dynamic
0.18 - 0.22
v = 1 m/s
0.20 - 0.23
v = 1.9 m/s
Abrasion
4.0
mm of depth after 70 hrs load duration; Partner Material ST 50
Electrical Properties
Original Value
Comments
Volume Resistivity
1.00e+11
ohm-cm
DIN 53482
Surface Resistance
1.00e+12
ohm
DIN 53482
Thermal Properties
Original Value
Comments
CTE, linear
110
µm/m-°C
@Temperature 100 °C
DIN 52328
Thermal Conductivity
0.930
W/m-K
DIN 52612
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Ensinger Tecatron® XP-83 Compression Molded PPS Compound, Filled with 10% PTFE, 10% Graphite and 15% Carbon Fiber
Ensinger TECASINT™ 2062 Polyimide, Anthrazit Gleamy, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT™ 2061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
Ensinger TECASINT 3062 Polyimide, Shiny Black, 15% Graphite, 10% PTFE (PI)
Ensinger TECASINT 1061 Polyimide, 15% Graphite, 10% PTFE Filled (PI)
PTEKU4 / 70057
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.