MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Morflo 170 Plus CR Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Calcined Bauxite raw material base. Hydraulic bond. A low cement, high fluidity, bauxite based 1700°C castable with high strengths at all temperatures, low porosity and excellent abrasion, impact and slag resistance.

Applications:

  • Forge furnace hearths
  • Door jambs, lintels and piers
  • Cartops
  • Rotary kiln nose rings, retainer rings and dams
  • Rotary hearth curbs
  • Walking beam furnace hearth, pusher furnace hearths
  • Skid pipe protection

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 2.78 g/ccdried to 110°C
Grain Size <= 6000 µm
 
Mechanical PropertiesOriginal ValueComments
Compressive Strength 120 - 200 MPaCold Crushing Strength
 80.0 - 140 MPa
@Treatment Temp. 110 °C
Cold Crushing Strength
 80.0 - 140 MPa
@Treatment Temp. 815 °C
Cold Crushing Strength
 120 - 200 MPa
@Treatment Temp. 1000 °C
Cold Crushing Strength
Abrasion >= 6.0
@Temperature 815 °C
cm3; ASTM C704
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 2.30 W/m-K
@Temperature 600 °C
Maximum Service Temperature, Air <= 1700 °C
Shrinkage 0.00 - 0.20 %
@Treatment Temp. 110 °C
 0.20 %
@Treatment Temp. 815 °C
 0.30 %
@Treatment Temp. 1000 °C
 1.0 %
@Treatment Temp. 1600 °C
 
Component Elements PropertiesOriginal ValueComments
Al2O3 79 %
CaO 1.8 %
Cr2O3 2.0 %
Fe2O3 1.3 %
K2O+Na2O 0.30 %Na2O + K2O
MgO 0.40 %
SiO2 13 %
TiO2 2.8 %
 
Descriptive Properties
Net Material Required (kg/m³)2780
Water Addition5.7-6.7 % by weight, 1.425-1.675 L per bag, 25 kg bag weight.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CMORF6367 / 203151

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.