MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Chase Electronic Coatings HumiSeal® 1B18 Acrylic Conformal Coating
Categories: Polymer; Thermoset

Material Notes: HumiSeal® 1B18 is a single component, fast drying, acrylic conformal coating intended for use on printed circuit assemblies. HumiSeal® 1B18 demonstrates excellent flexibility and electrical properties, fluoresces under UV light for ease of inspection and is easily repaired. HumiSeal® 1B18 coating is RoHS Directive 2002/95/EC compliant, and recognized under UL File Number E105698.

Information provided by Chase Electronic Coatings.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.920 g/cc0.0332 lb/in³ASTM D1475
Solids Content 30 %30 %± 2%. By weight; Fed-Std-141, Meth. 4044
Volatile Organic Compounds (VOC) Content 654 g/l654 g/l
Viscosity 230 - 270 cP230 - 270 cPFed-Std-141, Meth. 4287
Thickness 25.0 - 75.0 microns0.984 - 2.95 milRecommended coating
 
Mechanical PropertiesMetricEnglishComments
Modulus of Elasticity 0.0111 GPa1.61 ksiDMA
 
Electrical PropertiesMetricEnglishComments
Insulation Resistance 7.00e+10 ohm7.00e+10 ohmMoisture; MIL-I-46058C
 5.50e+14 ohm5.50e+14 ohmMIL-I-46058C
Dielectric Constant >= 2.6
@Frequency 1e+6 Hz,
Temperature 25.0 °C
>= 2.6
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
Dielectric Breakdown 6300 V6300 VASTM D149
Dissipation Factor 0.010
@Frequency 1e+6 Hz,
Temperature 25.0 °C
0.010
@Frequency 1e+6 Hz,
Temperature 77.0 °F
ASTM D150-98
 
Thermal PropertiesMetricEnglishComments
CTE, linear 67.0 µm/m-°C37.2 µin/in-°FTMA
Glass Transition Temp, Tg 42.0 °C108 °FDSC
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 min
@Temperature 76.0 °C
0.500 hour
@Temperature 169 °F
Option
 1440 min
@Temperature 23.0 °C
24.0 hour
@Temperature 73.4 °F
Option
 10100 min
@Temperature 23.0 °C
168 hour
@Temperature 73.4 °F
Optimum Properties
Tack-Free Time 30.0 min0.500 hourTo handle; Fed-Std-141, Meth. 4061
Shelf Life 24.0 Month
@Temperature 23.0 °C
24.0 Month
@Temperature 73.4 °F
DOM
 
Descriptive Properties
Dielectric Withstand>1500 Vper MIL_I_46058C
Fungus ResistancePassesASTM G21
Thermal Shock-65 to 125°Cper MIL_I_46058C, 50 cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCHAS902 / 239763

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.