MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Domo TECHNYL® SSD 330 KNF/E PA66, 15% glass filled, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Description: Polyamide 66, reinforced with 33% of glass fiber, for injection molding specially stabilized to improves its resistance to automotive cooling liquids.

Available in: Asia Pacific

Product Applications: TECHNYL® SSD 330 KNF/E is particularly recommended for the injection molding of parts in permanent contact with cooling liquids in cars, such as: cooling and heating radiator systems, header tanks, thermostat components, and inlet/outlet pipes. This product is available in Black and in color on request.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.39 g/ccISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 121ASTM D786
Tensile Strength, Yield 195 MPaASTM D638
Elongation at Break 3.0 %ASTM D638
Flexural Strength 300 MPaASTM D790
Flexural Modulus 10300 MPaASTM D790
Izod Impact, Notched 120 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 23.0 µm/m-°C
@Temperature 23.0 - 85.0 °C
ISO 11359
Melting Point 262 °CASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 255 °CISO 75/Af
Oxygen Index 23 %ISO 4589
Glow Wire Flammability Index 650 °C
@Thickness 1.60 mm
ISO 60695-2-12
 
Processing PropertiesOriginal ValueComments
Feed Temperature 270 - 280 °C
Mold Temperature 70.0 - 100 °C
Drying Temperature 80.0 °C
Moisture Content <= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PRHOD804 / 138035

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.