MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Matexcel NAT-151 Hyaluronic acid sodium salt from Streptococcus equi, 70-120KDa
Categories: Wood and Natural Products

Material Notes: This product is isolated from Streptococcus equi and it is suitable for cell biology, tissue engineering, cell culture, and enzyme characterization research.

Application: Hyaluronic acid, an anionic, nonsulfated glycosaminoglycan (GAG), may be used in research involving processes such as inflammation, cell signaling, cell migration, cell differentiation, tissue engineering and wound-healing. Hyaluronic acid may be used as a substrate to identify and characterized catabolizing enzymes such as hyaluronidase(s). Hyaluronic acid may be used in biomaterials research for the development of biological scaffolds for wound-healing applications and hyaluronic acid fillers in human skin.

Morphology: White powder

Key Words: Synonyms: HA, Hyaluronan, Hyaluronate, Sodium hyaluronate, Poly(b-glucuronic acid-[1?3]-b-N-acetylglucosamine-[1?4]); a-?UA-(1?10)-GlcNAc; sodium hyaluronate powder, hyaluronic acid; hyalobarrier gel; haluronic acid; hyaluronic acid sodium; hyaluronic acid na-salt;
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Molecular Weight 70000 - 120000 g/mol70000 - 120000 g/mol
Storage Temperature -20.0 °C-4.00 °F
 
Descriptive Properties
CAS Number9067-32-7

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMXCK1240 / 299871

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.