MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Metalmen Sales

Kennametal Stellite Stellite® 31 PM cast
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Typical applications include vane plugs, fuel metering pins, spacer bushings, ball bearing blanks, race bearing blanks, diesel engine exhaust, fluid valve seats, saw cutter inserts, miscellaneous wear parts. Data provided by the manufacturer, Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.45 g/cc0.305 lb/in³P/M (98%)
 8.61 g/cc0.311 lb/in³Theoretical
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 745 MPa108000 psi
 436 MPa
@Temperature 760 °C
63200 psi
@Temperature 1400 °F
 521 MPa
@Temperature 649 °C
75600 psi
@Temperature 1200 °F
 552 MPa
@Temperature 538 °C
80100 psi
@Temperature 1000 °F
Tensile Strength, Yield 526 MPa
@Strain 0.2 %
76300 psi
@Strain 0.2 %
 280 MPa
@Strain 0.2 %,
Temperature 538 °C
40600 psi
@Strain 0.2 %,
Temperature 1000 °F
Elongation at Break 9.0 %9.0 %in 25.4 mm
 12 %
@Temperature 649 °C
12 %
@Temperature 1200 °F
in 25.4 mm
 15 %
@Temperature 760 °C
15 %
@Temperature 1400 °F
in 25.4 mm
 18 %
@Temperature 538 °C
18 %
@Temperature 1000 °F
in 25.4 mm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.1 µm/m-°C
@Temperature 21.0 - 316 °C
7.83 µin/in-°F
@Temperature 69.8 - 601 °F
 14.5 µm/m-°C
@Temperature 21.0 - 427 °C
8.06 µin/in-°F
@Temperature 69.8 - 801 °F
 15.1 µm/m-°C
@Temperature 21.0 - 538 °C
8.39 µin/in-°F
@Temperature 69.8 - 1000 °F
 15.7 µm/m-°C
@Temperature 21.1 - 649 °C
8.72 µin/in-°F
@Temperature 70.0 - 1200 °F
 16.5 µm/m-°C
@Temperature 21.1 - 816 °C
9.17 µin/in-°F
@Temperature 70.0 - 1500 °F
 16.6 µm/m-°C
@Temperature 21.1 - 871 °C
9.22 µin/in-°F
@Temperature 70.0 - 1600 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.50 %0.50 %
Chromium, Cr 25.5 %25.5 %
Cobalt, Co 50 %50 %As remainder
Iron, Fe <= 2.0 %<= 2.0 %
Manganese, Mn <= 1.0 %<= 1.0 %
Nickel, Ni 10.5 %10.5 %
Other <= 2.0 %<= 2.0 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.040 %<= 0.040 %
Tungsten, W 7.5 %7.5 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 6 PM cast
Kennametal Stellite Deloro® 208 PM cast
Kennametal Stellite Stellite® 21
Kennametal Stellite Stellite® 31 PM after P/M processing, aged 8 hours at 802°C air cooled
Kennametal Stellite Stellite® 12 PM cast

NS31PB / 18862

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.