MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Sandvik 5R75 Seamless tube and pipe
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: Austenitic stainless steel, AISI type 316Ti

Sandvik 5R75 is an austenitic, titanium-stabilized stainless chromium–nickel–molybdenum steel.

Information provided by Sandvik

ASTM 316Ti; UNS S31635; EN 1.4571

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Vickers 155
Tensile Strength, Ultimate 510 - 710 MPa
Tensile Strength, Yield >= 220 MPa
@Strain 0.2 %
 >= 250 MPa
@Strain 1 %
 >= 127 MPa
@Strain 0.2 %,
Temperature 550 °C
 >= 129 MPa
@Strain 0.2 %,
Temperature 500 °C
 >= 132 MPa
@Strain 0.2 %,
Temperature 450 °C
 >= 136 MPa
@Strain 0.2 %,
Temperature 400 °C
 >= 140 MPa
@Strain 0.2 %,
Temperature 350 °C
 >= 145 MPa
@Strain 0.2 %,
Temperature 300 °C
 >= 157 MPa
@Strain 1 %,
Temperature 550 °C
 >= 157 MPa
@Strain 0.2 %,
Temperature 250 °C
 >= 164 MPa
@Strain 1 %,
Temperature 500 °C
 >= 167 MPa
@Strain 1 %,
Temperature 450 °C
 >= 167 MPa
@Strain 0.2 %,
Temperature 200 °C
 >= 171 MPa
@Strain 1 %,
Temperature 400 °C
 >= 175 MPa
@Strain 1 %,
Temperature 350 °C
 >= 177 MPa
@Strain 0.2 %,
Temperature 150 °C
 >= 180 MPa
@Strain 1 %,
Temperature 300 °C
 >= 185 MPa
@Strain 0.2 %,
Temperature 100 °C
 >= 186 MPa
@Strain 1 %,
Temperature 250 °C
 >= 196 MPa
@Strain 1 %,
Temperature 200 °C
 >= 202 MPa
@Strain 0.2 %,
Temperature 50.0 °C
 >= 206 MPa
@Strain 1 %,
Temperature 150 °C
 >= 218 MPa
@Strain 1 %,
Temperature 100 °C
 >= 234 MPa
@Strain 1 %,
Temperature 50.0 °C
Elongation at Break >= 35 %
Modulus of Elasticity 200 GPa
 165 GPa
@Temperature 500 °C
 172 GPa
@Temperature 400 °C
 179 GPa
@Temperature 200 °C
 179 GPa
@Temperature 300 °C
 194 GPa
@Temperature 100 °C
Charpy Impact 60.0 J
@Temperature -196 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 16.5 µm/m-°C
@Temperature 30.0 - 100 °C
 17.0 µm/m-°C
@Temperature 30.0 - 200 °C
 17.5 µm/m-°C
@Temperature 30.0 - 300 °C
 18.0 µm/m-°C
@Temperature 30.0 - 400 °C
 18.0 µm/m-°C
@Temperature 30.0 - 500 °C
 18.5 µm/m-°C
@Temperature 30.0 - 500 °C
 19.0 µm/m-°C
@Temperature 30.0 - 700 °C
Specific Heat Capacity 0.485 J/g-°C
@Temperature 20.0 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.500 J/g-°C
@Temperature 100 °C
 0.515 J/g-°C
@Temperature 200 °C
 0.525 J/g-°C
@Temperature 300 °C
 0.525 J/g-°C
@Temperature 300 °C
 0.540 J/g-°C
@Temperature 400 °C
 0.555 J/g-°C
@Temperature 500 °C
 0.555 J/g-°C
@Temperature 500 °C
 0.575 J/g-°C
@Temperature 600 °C
Thermal Conductivity 14.0 W/m-K
@Temperature 20.0 °C
 15.0 W/m-K
@Temperature 100 °C
 17.0 W/m-K
@Temperature 200 °C
 18.0 W/m-K
@Temperature 300 °C
 20.0 W/m-K
@Temperature 400 °C
 21.0 W/m-K
@Temperature 500 °C
 23.0 W/m-K
@Temperature 600 °C
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.050 %
Chromium, Cr 17 %
Iron, Fe 66.7 %As Balance
Manganese, Mn 1.3 %
Molybdenum, Mo 2.1 %
Nickel, Ni 12 %
Phosphorus, P <= 0.030 %
Silicon, Si 0.50 %
Sulfur, S <= 0.030 %
Titanium, Ti >= 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Sandvik 316Ti-5R75 Billet
Sandvik 316Ti-8LR70 Billet
AISI Type 410S Stainless Steel, tempered at 343°C
Outokumpu 4301 Cr-Ni Austenitic Stainless Steel
316 Stainless Steel, annealed sheet

NSANDV242 / 19136

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.