MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total Finathene® WR 201 B N HDPE blow molding  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Blow Molding Grade

Material Notes: FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process.

FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel Tanks and automotive technical parts.

FINATHENE® WR 201 B N is suitable for the most common barrier treatments. The material specific characteristics allow to achieve outstanding tank properties, including crash test and fire resistance, with a substantial net weight reduction of the Plastic Fuel Tank.

Information provided provided by Total Petrochemicals.

Total Petrochemicals includes former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.9495 g/ccISO 1183
Environmental Stress Crack Resistance >= 360 hourASTM D1693 cond. B 100% lgepal
Thermal Stress Crack Resistance >= 250 hourASTM D 1693
High Load Melt Index 8.0 g/10 min
@Load 21.6 kg
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 25.0 MPaISO 527
Elongation at Yield 11 %ISO 527
Flexural Modulus 1.10 GPaISO 178
Impact Test 20.0 JMultiaxial, @ ULT, deflection = 14 mm; ASTM D 3763
 
Thermal PropertiesOriginal ValueComments
Melting Point 127 °CASTM D3417

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Braskem HB 0155 HDPE Blow Molding Polyethylene
Overview of materials for High Density Polyethylene (HDPE), Blow Molding Grade
Kolon SPESIN® KP513UG PBT Alloy Resin
Total Finathene® WR 201 B HDPE blow molding
Total 51090 High Density Polyethylene - Blow Molding

PFINAP075 / 38658

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.