MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Domo TECHNYL® CR 218 V33 Black 21 N Nylon 6, 30% glass fiber, DRY
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 30% Glass Fiber Filled

Material Notes: Description: Polyamide PA6 reinforced with 33% of glass fiber, heat stabilized, containing recycled material.

Available in: North America

Product Applications: This grade is suitable for none critical and less demanding parts. This product is available in black. This product can only be used in line with the specific recommendations of the Rhodia Engineering Plastics customer technical service. Rhodia Engineering Plastics declines all responsibilities for all problems caused by the use of this product, not in line with the recommendations of Rhodia Engineering Plastics customer technical service

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 189.3 MPa27460 psiISO 527 Type 1A
Elongation at Break 3.3 %3.3 %ISO 527 Type 1A
Tensile Modulus 10.7 GPa1550 ksiISO 527 Type 1A
Flexural Strength 285 MPa41300 psiISO 178
Flexural Modulus 9.088 GPa1318 ksiISO 178
Izod Impact, Notched (ISO) 15.5 kJ/m²7.38 ft-lb/in²ISO 180/1A
Izod Impact, Unnotched (ISO) NBNBISO 180/1U
Charpy Impact Unnotched NBNBISO 179/1eU
 
Processing PropertiesMetricEnglishComments
Feed Temperature 230 - 235 °C446 - 455 °F
Mold Temperature 60.0 - 90.0 °C140 - 194 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-250°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo Technyl® C216V30 30% Glass Filled Nylon 6
Domo TECHNYL® eXten D218 V30 Nylon 6.10, 30% glass fiber, DRY
Domo Technyl® A 205F Nylon 66, EH0
Domo TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Domo TECHNYL® 2710IR PA66, DRY

PRHOD550 / 137781

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.