MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Grade 702 Zirconium, Commercially Pure
Categories: Metal; Nonferrous Metal; Zirconium Alloy; Pure Element

Material Notes: Characteristics:
  • Ductile
  • Mechanical Properties similar to titanium and austenitic stainless steel
  • Excellent corrosion resistance
  • Forms stable oxide layer
  • Highly anisotropic

Applications: Chemical processing equipment

Machining Parameters: Use slow speeds, heavy feeds and flood cooling with a water-soluble oil lubricant

Key Words: UNS R60702, Zircadyne® 702
Vendors: Eagle Alloys Corporation is a leading supplier of quality metals and alloys. Our staff prides itself on working fast, efficiently and courteously to get you the information you need. Call (800) 237-9012 or visit www.EagleAlloys.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 6.50 g/cc
Vapor Pressure 0.0100 torr
@Temperature 2000 °C
 900 torr
@Temperature 3600 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell A 49Estimated from Vickers
Hardness, Rockwell B 78Estimated from Vickers
Hardness, Vickers 150Annealed Sample
Tensile Strength, Ultimate >= 379 MPa
 140 MPa
@Temperature 400 °C
 205 MPa
@Temperature 300 °C
 230 MPa
@Temperature 200 °C
 350 MPa
@Temperature 100 °C
 450 MPa
@Temperature 20.0 °C
Tensile Strength, Yield 80.0 MPa
@Temperature 400 °C
 90.0 MPa
@Temperature 300 °C
 150 MPa
@Temperature 200 °C
 260 MPa
@Temperature 100 °C
 325 MPa
@Temperature 20.0 °C
 >= 207 MPa
@Strain 0.2 %
Elongation at Break 16 %in 50 mm
 21 %
@Temperature 400 °C
 32 %
@Temperature 20.0 °C
 38 %
@Temperature 100 °C
 50 %
@Temperature 300 °C
 56 %
@Temperature 230 °C
Modulus of Elasticity 99.3 GPa
Poissons Ratio 0.35
Fatigue Strength 60.0 MPa
@# of Cycles 3.00e+7
notched
 125 MPa
@# of Cycles 500000
notched
 145 MPa
@# of Cycles 3.00e+7
unnotched
 175 MPa
@# of Cycles 5000
unnotched
Shear Modulus 36.2 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.0000397 ohm-cmTemp Coefficient is 0.0044/°C at 20°C
Magnetic Susceptibility 0.00000134cgs/g; pure Zr
Critical Magnetic Field Strength, Oersted 47Pure Zr
Critical Superconducting Temperature 0.595 - 0.625 Kpure Zr
 
Thermal PropertiesOriginal ValueComments
Heat of Fusion 250 J/g
Heat of Vaporization 6490 J/g
CTE, linear 5.89 µm/m-°C
@Temperature 25.0 °C
 6.30 µm/m-°C
@Temperature 250 °C
 6.90 µm/m-°C
@Temperature 500 °C
Specific Heat Capacity 0.285 J/g-°C
Thermal Conductivity 22.0 W/m-K
Melting Point 1852 °C
Boiling Point 4377 °C
 
Optical PropertiesOriginal ValueComments
Emissivity (0-1) 0.32650 nm; unoxidized pure Zr sample; total
 
Component Elements PropertiesOriginal ValueComments
Fe + Cr 0.20 %
Hafnium, Hf <= 4.5 %
Oxygen, O 0.16 %
Zirconium, Zr >= 99.2 %includes Hf
 
Descriptive Properties
Alpha Phase Crystal Structurehcp< 865°C
Beta Phase Crystal Structurebcc> 865°C

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Grade 705 Zirconium (Zr-2.5Nb)
Zircaloy-4 Zirconium Alloy
Reactor Grade Zirconium
Zirconium, Zr
Zr-2.5Nb Zirconium Alloy, Nuclear Grade

MZRI00 / 14570

Metalmen Sales

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.